Fixation of heavy metals, mercury recovery and dioxins destruction in municipal solid waste incinerator ash
AssigneeAir Products and Chemicals, Inc.
InventorsWolfgang A. Hochleitner, Stephen P. Goff
Life of this patent
Estimating the term…
Loading patent…
AssigneeAir Products and Chemicals, Inc.
InventorsWolfgang A. Hochleitner, Stephen P. Goff
Estimating the term…
Fly ash generated from incineration of municipal solid waste (MSW) when placed in landfills can under mild acid conditions 1each lead and cadmium. A process for stabilizing lead in this fly ash is presented which involves calcining a mixture of the fly ash and certain calcium-containing compounds in the presence of an oxygen containing gas stream at a temperature greater than about 475.degree. C. and less than about 600.degree. C. for times from about 30 minutes up to about 5 hours. Such treated MSW fly ash will give leachates containing lead concentrations less than the EPA regulatory limit.
In a process for the stabilization of heavy metals-containing fly ash obtained by subjecting flue gas to particulate separation, which process comprises forming a mixture of the fly ash and a calcium-containing material, said calcium-containing material being present in the mixture so as to provide a weight ratio of calcium to fly ash from about 0.04 to about 0.5:1, heating the mixture to a temperature in the range of from about 475.degree. C. to about 650.degree. C. and maintaining said temperature for a period of time from about 30 minutes to about five hours while in the presence of an oxygen-containing gas to produce a thermally treated fly ash and a purge gas, the improvement for (1) volatilizing and subsequently recovering any mercury which may be contained in the fly ash;
Dependencies are inferred from the claim text.