Polynuclear complex salt waste water clarificants and their preparation
AssigneesTadahiko Kuno, Jun-ichi Hosokawa, Toko Abasu Co., Ltd.
InventorTadahiko Kuno
Life of this patent
Estimating the term…
Loading patent…
AssigneesTadahiko Kuno, Jun-ichi Hosokawa, Toko Abasu Co., Ltd.
InventorTadahiko Kuno
Estimating the term…
A wastewater clarificant very excellent in the powers for removing BOD, COD and SS is provided. The clarificant comprises an aqueous solution containing a polynuclear complex salt that is obtained by subjecting to isochoric heating an aqueous solution containing a mixture of sulfates of a plurality of metals selected from the group consisting of potassium, iron, calcium, sodium, magnesium and aluminum. Preferably, the clarificant comprises an aqueous solution containing a polynuclear complex salt that is obtained by subjecting to isochoric heating an aqueous solution containing a mixture of sulfates of a plurality of metals selected from the group consisting of, in molar concentration, 0.02 to 0.08 of potassium, 0.11 to 1.31 of iron, 0.003 to 0.030 of calcium, 0.004 to 0.040 of sodium, 0.27 to 0.81 of magnesium and 0.370 to 1.300 of aluminum.
A wastewater clarificant containing a polynuclear complex salt comprising sulfates of potassium, iron, calcium, sodium, magnesium and aluminum, obtained by heating and pressurizing at 100.degree. C. to 190.degree. C. and 1 kgf/cm.sup.2, an aqueous solution containing a mixture of said sulfates.
A wastewater clarificant comprising an aqueous solution containing a polynuclear complex salt that is obtained by subjecting to heating and pressurizing at 100.degree. C. to 190.degree. C. and 1 kgf/cm.sup.2 to 10.0 kgf/cm.sup.2 an aqueous solution containing a mixture of sulfates of potassium, iron, calcium, sodium, magnesium and aluminum.
A wastewater clarificant comprising an aqueous solution containing a polynuclear complex salt that is obtained by subjecting to heating and pressurizing at 100.degree. C. to 190.degree. C. and 1 kgf/cm.sup.2 to 10.0 kgf/cm.sup.2 an aqueous solution containing a mixture of sulfates of, in molar concentration, 0.02 to 0.08 of potassium, 0.11 to 1.31 of iron, 0.003 to 0.030 of calcium, 0.004 to 0.040 of sodium, 0.27 to 0.81 of magnesium and 0.370 to 1.300 of aluminum.
A wastewater clarificant comprising an aqueous solution containing a polynuclear complex salt comprising sulfates of a plurality of metals, which contains per 1 liter 0.78 to 5.63 g of potassium ions, 6.00 to 73.00 g of iron ions, 0.12 to 1.20 g of calcium ions, 0.10 to 1.00 g of sodium ions, 6.56 to 19.70 g of magnesium ions, 6.21 to 35.00 g of aluminum ions and 106.08 to 463.77 g of sulfuric ions.
A method for preparing a wastewater clarificant comprising an aqueous solution containing a polynuclear complex salt by subjecting to heating and pressuring at 100.degree. C. to 190.degree. C. and 1 kgf/cm.sup.2 to 10.0 kgf/cm.sup.2 an aqueous solution containing sulfates of a plurality of metals, which contains per 1 liter 0.78 to 5.63 g of potassium ions, 6.00 to 80.00 g of iron ions, 0.12 to 1.20 g of calcium ions, 0.10 to 1.00 g of sodium ions, 6.56 to 19.70 g of magnesium ions, 6.21 to 35.00 g of aluminum ions and 106.08 to 463.77 g of sulfuric ions.
Dependencies are inferred from the claim text.