A color development process for processing an imagewise exposed silver halide color photographic material comprising a support having thereon at least one light-sensitive silver halide emulsion layer comprising a color coupler and a silver iodobromide emulsion containing silver iodide in an amount of from 2 to 20 mol %, comprising the step of processing the color photographic material in a color developing solution containing a color developing agent and bromide ion for 40 seconds to 90 seconds, wherein the color developing agent is represented by formula (D'):
- ##STR19## where R.sub.1d, R.sub.2d, each represents an alkyl group having 1 to 4 carbon atoms;
- and L.sub.1 represents a straight-chain or branched alkylene group having 3 or 4 carbon atoms;
- the concentration {Br.sup.- } of bromide ion in the color developing solution is from 30 to 60 mmol/l;
- the relationship between the concentration {R} of the color developing agent in the color developing solution and the concentration {Br.sup.- } of bromide ion in the color developing solution and the relationship between the development processing temperature Tem and the concentration {Br.sup.- } of bromide ion are maintained to satisfy a Rule defined by the following equations:
- (Rule)
- {R}=((0.63.times.{Br.sup.- })+(14)).+-.16 (mmol/l)
- Tem=((0.19.times.{Br.sup.- })+(39)).+-.5 (.degree.C.)
- where {R} is the concentration of color developing agent in units of mmol/l;
- {Br.sup.- } is the concentration of bromide ion in units of mmol/l;
- and
- Tem is the development processing temperature in .degree.C.