Light-sensitive composition and process
AssigneeShipley Company, L.L.C.
InventorsGeorge R. E. Daniels, Michael J. Oddi, Kevin J. Cheetham, Stephen S. Rodriguez
Life of this patent
Estimating the term…
Abstract
A photoimageable composition and process for use of the same. The composition comprises a binder that is a mixture of a phenolic resin and a multifunctional epoxy or vinyl ether pound and a curing system comprising a photoactive compound capable of generating a curing catalyst capable of crosslinking the binder components. The process for use of the composition comprises application of the composition to a substrate, drying of the same, exposing the dried coating to activating radiation, curing the binder in light exposed areas, developing the coating and thermally curing the developed image. The composition is especially useful as a solder mask.
Claims25
An aqueous developable photoimageable composition comprising a binder and a curing system for components of said binder, said binder comprising an admixture of a phenolic resin and a compound having at least two reactive functionalities selected from the group of an epoxy radical, a vinyl ether radical and a mixture of an epoxy and a vinyl ether radical, and said curing system comprising a crosslinking agent for the phenolic resin and photoactive compound capable of generating a curing catalyst for said binder;
- said phenolic resin being present in an amount sufficient to render unexposed portions of the composition alkali soluble, said compound having at least two reactive functionalities being present in an amount capable of hardening said composition, and said curing system being present in a amount capable of curing the components of the binder upon exposure to activating radiation and baking before development.
An aqueous developable photoimageable composition comprising an admixture of a phenolic resin, an epoxy resin, an onium salt and the product of reaction of formaldehyde and melamine, said components being present in the following amounts in parts by weight:
- ______________________________________ phenolic resin 25-65 epoxy resin 15-50 melamine resin 5-35 onium salt 1-15. ______________________________________
Dependencies are inferred from the claim text.