Oxygen absorbent composition and method of preserving article with same
AssigneeMitsubishi Gas Chemical Company, Inc.
InventorsYoshiaki Inoue, Shigeru Murabayashi, Kazuo Fujinami, Isamu Yoshino, Akira Naito
Life of this patent
Estimating the term…
Abstract
An oxygen absorbent composition containing a linear hydrocarbon polymer having one or more unsaturated groups or a mixture of a linear hydrocarbon polymer having one or more unsaturated groups with an unsaturated fatty acid compound and an oxidation promoter as essential components and optionally containing a basic substance and/or an adsorption substance; an oxygen absorbent parcel formed by packing the oxygen absorbent composition with a gas-permeable packing material; and a method of preserving an article by means of same.
Claims6
An oxygen absorbent composition, comprising:
- a polymer selected from the group consisting of polymers of isoprene, butadiene, 1,3-pentadiene and squalene, or a mixture of said polymer with an unsaturated fatty acid compound;
- 0.1 to 75 parts by weight per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of an oxidation promoter selected from the group consisting of transition metals and transition metal compounds;
- 0.1 to 1,000 parts by weight, per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of a basic substance selected from the group consisting of oxides, hydroxides, carbonates, organic acid salts of alkali metals and alkaline earth metals and amine compounds;
- and
- 50 to 1,000 parts by weight, per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of an adsorption substance selected from the group consisting of silica gel, activated clay, diatomaceous earth, zeolite, activated carbon, and pearlite.
An oxygen absorbent composition comprising
- a polymer selected from the group consisting of polymers of isoprene, butadiene, 1,3-pentadiene and squalene, or a mixture of said polymer with an unsaturated fatty acid compound;
- and
- 0. 1 to 75 parts by weight per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of an oxidation promoter selected from the group consisting of transition metals and transition metal compounds;
- 0.1 to 10 parts by weight, per 100 parts by weight of the composition, of a humidity adjusting agent having a viscosity, at 20.degree. to 50.degree. C., of not more than 10.sup.4 cp and an equilibrium relative humidity of not more than 70%, said humidity adjusting agent providing an equilibrium relative humidity of 20 to 70% in an enclosed system,
- 0.1 to 1,000 parts by weight, per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of a basic substance selected from the group consisting of oxides, hydroxides, carbonates, organic acid salts of alkali metals and alkaline earth metals and amine compounds;
- and
- 50 to 1,000 parts by weight, per 100 parts by weight of the polymer or the mixture of the polymer with the unsaturated fatty acid compound, of an adsorption substance selected from the group consisting of silica gel, activated clay, diatomaceous earth, zeolite, activated carbon, and pearlite.
Dependencies are inferred from the claim text.