US 4,810,314 AGranted
Enhanced corrosion resistant amorphous metal alloy coatings
AssigneeThe Standard Oil Company
InventorsRichard S. Henderson, Gary A. Shreve, Michael A. Tenhover
Life of this patent
Estimating the term…
Abstract
The present invention relates to an amorphous metal alloys of the formula: Cr.sub.a X.sub.b M.sub.c wherein X is at least one element selected from the group consisting of Pt, Pd, Ir, Rh and Ru; M is at least one element selected from the group consisting of P, B, N, C, As, Sb and S; and wherein a ranges from about 0.60 to abotu 0.96; b ranges from greater than zero to about 0.01; c ranges from about 0.04 to about 0.40; and with the provisor that a+b+c equals 1.00.
Claims7
An amorphous metal alloy of the formula is:
- Cr.sub.a X.sub.b M.sub.c
- wherein
- X is at least one element selected from the group consisting of:
- Pt, Pd, Ir, Rh and Ru;
- M is at least one element selected from the group consisting of P, B, N, C, As, Sb and S;
- and wherein
- a ranges from about 0.69 to about 0.96;
- b ranges from greater than zero to about 0.01;
- c ranges from about 0.04 to about 0.40;
- and with the proviso that a+b+c equals 1.00.
7 more elements
An amorphous metal alloy coating of the formula:
- Cr.sub.a X.sub.b M.sub.c
- wherein
- X is at least one element selected from the group consisting of
- Pt, Pd, Ir, Rh and Ru;
- wherein
- M is at least one element selected from the group consisting of P, B, N, C, As, Sb and S;
- and wherein
- a ranges from about 0.69 to 0.96;
- b ranges from greater than zero to about 0.01;
- c ranges from about 0.04 to about 0.40;
- and with the proviso that a+b+c equals 1.00, formed by a process comprising depositing a film of said amorphous metal alloy on a substrate.