Process for making ferrite spherical particulate toner core from raw fly ash
AssigneeHalomet, Incorporated
InventorsRobert G. Aldrich, Geoffrey H. Earl, David W. Trunko
Life of this patent
Estimating the term…
Loading patent…
AssigneeHalomet, Incorporated
InventorsRobert G. Aldrich, Geoffrey H. Earl, David W. Trunko
Estimating the term…
A process for making a ferrite spherical particulate toner carrier core from a raw fly ash comprising recovering the magnetic particles from the non-magnetic particles of the raw fly ash; selecting a desired size for the particles of the raw fly ash and screening the fly ash to obtain the desired sized particles; and purifying the resultant raw fly ash to obtain a ferrite composition having a particle size from 20-300 microns, in which the particles are essentially spherical, having an apparent density of at least 1.8 g/cm.sup.3, a saturation magnetization of 43-70 emu/g, a remanence of 5 emu/g or less, a Hall Flow of 20 sec. or greater/50 g.
A process for making a ferrite spherical particulate toner carrier core from raw fly ash obtained from burning coal comprising
Dependencies are inferred from the claim text.