Back to results
US 4,398,406 AGranted
Method for producing cold rolled titanium strips
AssigneeKabushiki Kaisha Kobe Seiko Sho
InventorsMasahito Fukuda, Akiyoshi Tanabe, Yasuo Moriguchi, Nobuyuki Nagai, Kunio Tsuji, Yoshihiro Yamaguchi, Tomiharu Matsushita, Atsuo Mizuta
Life of this patent
Estimating the term…
Abstract
A method for producing cold rolled titanium strips having good surface quality. The cold rolling of a titanium strip is carried out under the conditions represented by the following formula: X.ltoreq.(48673/Y.sup.1.3283) where X is an average grain size (.mu.m) of the pre-cold rolled titanium strip and Y is a diameter (mm) of the roll for the cold rolling.
Claims5
A method for producing a cold-rolled titanium strip, comprising:
- predetermining the average grain size in micrometers of a pre-cold-rolled titanium strip, and
- cold-rolling said pre-cold-rolled titanium strip under the condition such that
- X.ltoreq.48673/.sub.Y 1.3283
- wherein X is the average grain size in micrometers of the pre-cold-rolled titanium strip, and
- Y is the diameter in millimeters of the rolls used for cold-rolling.
2 more elements