Wear reducer
AssigneeThe United States of America as represented by the Secretary of the Army
InventorsSydney Axelrod, Walter Brenner, Barry A. Rugg
Life of this patent
Estimating the term…
Abstract
An improved ammunition propellant composition and method for reducing gun mber wear, erosion, flash and cook-off through use of an additive comprising a mixture of a super water absorbent starch modified polyacrylonitrile which has been subjected to alkaline saponification and water. The wear reducing additive is preferably formed into sheets which can be used with propellants selected from the group consisting of bagged propelling charges and cartridge cased propellants.
Claims5
A method for reducing gun member thermal erosion and wear through use of coolant additive with a propellant charge for reducing propellant flame temperature comprising the steps of preparing a sheet comprising a highly water adsorbent starch-acrylonitrile copolymer which has been subjected to alkaline saponification and a major amount of absorbed water;
- and disposing said sheet around the ammunition propellant charge to reduce erosion by formation of a laminar cooling layer of gas adjacent to the gun member upon firing of said charge.
Dependencies are inferred from the claim text.