Abstract
A process for making a pressure-sensitive adhesive coated product from an elastomer utilizing dry blending of powders and dry coating steps is described. Compositions suitable for use in this process are also described.
Claims6
A process for making a pressure-sensitive adhesive coated product comprising:
- (a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
- (b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
- (c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
- (d) dry coating said powder blend onto the surface of a substrate,
- (e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating, and
- (f) allowing to cool to ambient temperature.
3 more elements
A process for making a pressure-sensitive adhesive tape comprising:
- (a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
- (b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
- (c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
- (d) dry coating said powder blend onto the surface of a sheet of heat-insensitive tape backing as substrate,
- (e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating, and
- (f) allowing to cool to ambient temperature.
3 more elements
A process for making pressure-sensitive adhesive tape comprising:
- (a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
- (b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
- (c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
- (d) dry coating said powder blend onto the surface of a temporary substrate of carrier paper,
- (e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating,
- (f) allowing to cool to ambient temperature to obtain an adhesive film, and
- (g) transferring the adhesive to a heat-sensitive or porous tape backing.
4 more elements