Solid fuel use in small furnaces
AssigneeMobil Oil Corporation
InventorTsoung Y. Yan
Life of this patent
Estimating the term…
Abstract
A method is described for preparing a solid fuel, in either powder or briquette form, for use in small furnaces. The fuel has a relatively uniform heating value of 12,000-14,000 Btu per pound and is prepared by crushing and grinding coal to less than 200 mesh and drying and oxidizing the coal with a hot gas containing a trace of oxygen to a dried moisture content of 1-15%. Selected quantities of additives having approximately the same fineness are combined with the coals to minimize the effects of sulfur, to improve combustion and ash properties, to maintain fluidity of the solid fuel in powder form, to inhibit moisture pick-up, and to prevent auto-ignition and spontaneous combustion during storage of the solid fuel.
Claims12
A method for producing a solid fuel for small furnaces in powder form or in briquette form which has:
- (a) a uniform heat content of approximately 12,000-14,000 Btu per pound, (b) a sulfur content that is balanced with a scavenger for SO.sub.2 gas to enable stack gases from said small furnaces to meet EPA emission standards for SO.sub.2, (c) an ash that is soft, pliable, and non-sticking and that does not form "clinkers" while burning, (d) no tendency during normal storage conditions to undergo spontaneous combustion or auto-ignition, (e) adequate flow properties so that said fuel in powder form maintains fluidity and does not stick in the delivery system therefor, (f) insignificant tendency to pick up moisture during transportation or storage, (g) excellent ignition properties during cold weather starting in a cold furnace, and (h) excellent combustion properties for reducing carbon monoxide emission and soot formation and for improved heat recovery, which comprises the following steps:
- A. grinding a coal or mixture of coals having a heating value of about 12,000 to 14,000 Btu to a fineness below 200 mesh;
- B. drying the coal or coals with a hot gas, which is at 150.degree.-800.degree. F. and contains a trace amount of oxygen, to a dried moisture content of 1-15%;
- C. blending the coal or coals with at least one additive selected from each group set forth below;
- (1) an SO.sub.2 scavenger for minimizing the effects of sulfur in said coal selected from the group consisting of limestone, lime, dolomite, gypsum, calcium phosphate, bauxite, and mixtures thereof,
- (2) a combustion improver and ash modifier for imparting burning properties and for reducing corrosion, fouling, and ash slagging, selected from the group consisting of manganese dioxide, iron oxide, and manganese nodules.