US 2026/0307055 A1Published application
Copper silicate-based catalyst and preparation method therefor
AssigneeLG Chem, Ltd.
InventorsMyungji SUH, Tae Yun KIM, Sungshik EOM
Life of this patent
Estimating the term…
Abstract
A copper silicate-based catalyst according to an exemplary embodiment of the present application contains copper and silica, wherein the weight ratio of Cu:Si in the copper silicate-based catalyst is 30:70 to 70:30, and the Cu 2p binding energy of the copper silicate-based catalyst determined by XPS (X-ray photoelectron spectroscopy) analysis is 932 eV to 934 eV.
Claims12
A copper silicate-based catalyst comprising copper and silica, wherein
- a weight ratio of Cu:Si in the copper silicate-based catalyst is 30:70 to 70:30, and
- a Cu 2p binding energy of the copper silicate-based catalyst determined by XPS (X-ray photoelectron spectroscopy) analysis is 932 eV to 934 eV.