Abstract
This relates to a process for the polymerisation of siloxane polymers and copolymers, made by base catalysed ring-opening polymerisation of cyclosiloxane oligomers having six siloxane units per ring, using a sodium silanolate catalyst. It also relates to the siloxane polymers and copolymers, made by the process and their uses.
Claims13
A base catalysed process for the preparation of linear or branched siloxane polymers and copolymers, by the ring-opening polymerisation of cyclosiloxane oligomers having six siloxane units per ring having six
- units per molecule, wherein each R″ group per unit is the same or different and is an alkyl group having from 1 to 6 carbons;
- which base catalysed process comprises the steps of
- (a) introducing
- (a) said cyclosiloxane oligomers having six siloxane units per ring in an amount of from 50 to 99 wt. % of the starting ingredients with
- (ii) one or more end-blockers in an amount of from 1 to 50 wt. % of the starting ingredients and optionally
- (iii) a co-monomer selected from a linear organosiloxane co-monomer, a branched organosiloxane co-monomer or cyclosiloxane co-monomer wherein said cyclosiloxane co-monomer has from 3 to 10
- units per molecule, wherein each R8 group is the same or different and is selected from an alkenyl group, an alkynyl group, an aryl group, a fluoroalkyl such as trifluoropropyl or a perfluoroalkyl group and each R9 group is selected from an alkyl group having from 1 to 6 carbons or R8;
- said co-monomer (iii), when present, being present in an amount of from 1 to 50 wt. % of the starting ingredients;
- into a mixing vessel and mixing;
- (b) optionally introducing an organic solvent in an amount of up to 30 wt. % of the starting ingredients into the mixing vessel during or subsequent to step (a);
- (c) heating said starting ingredient (i) to a predetermined reaction temperature of from 25 to 175° C. in an inert atmosphere before introducing component (ii) and optionally component (iii), when present, or
- heating a mixture of starting ingredients (i), (ii) and optionally (iii) to a predetermined reaction temperature of from 25 to 175° C. in an inert atmosphere;
- (d) once the predetermined reaction temperature has been reached, and starting materials (i), (ii) and optionally (iii) are thoroughly mixed together, introducing a final starting ingredient, a sodium silanolate base catalyst (iv) of the structure R20—O− Na+ where R20 is an organopolysiloxane chain;
- in an amount of from 0.001 to 10 wt. % of the starting ingredients;
- thereby forming an initial reaction mixture;
- (e) agitating the initial reaction mixture at the predetermined reaction temperature for up to 24 hours until a step (e) product within a desired number average molecular weight range and/or a cyclics equilibration is obtained;
- (f) quenching the reaction after step (e) by either filtering off heterogeneous acid catalysts when used or by neutralising the step (e) product with a suitable acid to form a step (f) product;
- (g) Cooling the step (f) product to ambient temperature to form a cooled step (g) product and optionally,
- (h) Stripping volatile cyclosiloxanes the cooled step (f) product to give a final linear or branched siloxane polymer or copolymer.
16 more elements
13-15. (canceled)
Dependencies are inferred from the claim text.