A method for preparing a water-soluble polymer for oil drilling operations, wherein the water-soluble polymer is in powder form, by radically polymerizing at least two water-soluble, monoethylenically unsaturated monomers (A) and (B), the method comprising:
- i) adding an aqueous base fluid into a vessel,
- ii) adding at least one radical initiator into the vessel and dissolving the radical initiator(s) in the aqueous base fluid,
- iii) continuously dosing the monomers into the vessel, and
- iv) removing the obtained water-soluble polymer from the vessel and drying it,
- wherein the maximum temperature of the vessel is equal or less than 100° C. at any point during the method, and wherein
- monomer (A) is of the formula H2C═C(R1)—CO—X—R2, wherein R1 is H or CH3, X is O or NR3, wherein R3 is H or CH3, and R2 is a hydrocarbon group comprising at least one OH pendant group or a group of the formula —(CH2CH(R4)—O)nR5, wherein R4 and R5 are, independently, H or CH3, and n is chosen from 1 to 20, and wherein the amount of monomer (A) is 0.1 to 30 mol %, relating to the total of all monomers, and
- monomer (B) is a monomer different from (A), having the general formula H2C═C(R1)—R6, wherein R1 has the meaning as defined above, and R6 is a hydrophilic group, and wherein the amount of monomer (B) is 70 to 99.9 mol %, relating to the total of all monomers.