Superfast recharging zinc-based energy storage devices
AssigneeNanotech Energy, Inc.
InventorsMaher F. EL-KADY, Mir F. MOUSAVI, Haosen WANG
Life of this patent
Estimating the term…
Abstract
Provided herein are rechargeable aqueous Zn∥Ni energy storage devices that exhibit improved electrochemical performance high performance and super-long life. The combination of a high-performance Zn-based anode and an efficient Ni-based cathode herein, which aqueous battery chemistry with outstanding, form an energy storage device with high energy and power densities and cycling stability.
Claims90
An energy storage device comprising:
- (a) an anode comprising a bimetallic particle on a graphene scaffold, the bimetallic particle comprising ZnxM1-xCO3 nanoparticles, wherein M is iron, cobalt, aluminum, manganese, or any combination thereof, and wherein x is less than 1;
- (b) a cathode comprising a layered double hydroxide (LDH) nanotube;
- and
- (c) an electrolyte.
An energy storage device comprising:
- (a) an anode comprising bimetallic ZnxM1-xCO3 nanoparticles on a graphene scaffold, wherein M is manganese, and wherein x is less than 1;
- (b) a cathode comprising sulfidated Ni—Co—Fe layered double hydroxide nanotube;
- and
- (c) an electrolyte.
A method of forming an electrode, the method comprising:
- (a) forming a first solution comprising graphene oxide and a solvent;
- (b) adding zinc nitrate hexahydrate and manganese nitrate tetrahydrate to the first solution;
- (c) adding a reducing agent to the first solution to form a second solution;
- (d) heating the second solution;
- (e) cooling the second solution;
- (f) washing the second solution;
- and
- (g) freeze drying the second solution.
A method of forming an electrode, the method comprising:
- (a) synthesizing Ni—Co—Fe layer double hydroxide nanoplatelets;
- (b) heating the Ni—Co—Fe layer double hydroxide nanoplatelets;
- and
- (c) drying the Ni—Co—Fe layer double hydroxide nanoplatelets.
A method of applying regenerative voltage pulse to a zinc-based energy storage device to maintain or increase the initial capacity, the method comprising:
- after a sequence of at least 10 galvanostatic charge-discharge (GCD) cycles:
- (a) applying a first voltage pulse at a first voltage for a first period of time;
- (b) applying a second voltage pulse at a second voltage for a second period of time;
- (c) repeating (a) and (b) at least every 10 galvanostatic charge-discharge (GCD) cycles;
- and
- (d) maintaining 100% of the initial device capacity after about 100 galvanostatic charge-discharge (GCD) cycles.
Dependencies are inferred from the claim text.