Surface-treated steel sheet and method for manufacturing surface-treated steel sheet
AssigneeNippon Steel Corporation
InventorsYasuto GOTO, Kosuke KAWAMOTO
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Steel Corporation
InventorsYasuto GOTO, Kosuke KAWAMOTO
Estimating the term…
A surface-treated steel sheet according to one aspect of the present invention is a surface-treated steel sheet including: a base steel sheet; a Ni-containing layer disposed on a surface of the base steel sheet; and a Ni—W alloy layer disposed on a surface of the Ni-containing layer, wherein the Ni-containing layer includes an Fe-diffused alloy layer, and the surface-treated steel sheet includes a W depletion layer in a range from a surface of the Ni—W alloy layer to a depth of 10 nm. In a method for manufacturing a surface-treated steel sheet according to another aspect of the present invention, an atmospheric dew point in annealing is set to −25 to 5° C., a soaking time in the annealing is set to 10 to 180 seconds, and a maximum temperature in the annealing is set to 630 to 860° C.
A surface-treated steel sheet, comprising:
A method for manufacturing a surface-treated steel sheet comprising:
Dependencies are inferred from the claim text.