Back to results
US 2026/0234039 A1Published application
Tin oxide doped with bismuth and copper semiconductor material for wastewater treatment
AssigneeImam Abdulrahman Bin Faisal University
InventorImen MASSOUDI
Life of this patent
Estimating the term…
Abstract
A semiconductor material is described. The semiconductor material includes tin oxide, bismuth and copper, where the tin oxide is doped with the bismuth and the copper, and where the bismuth is present in an amount of 1 to 5 weight percent (wt. %) based on a total weight of the semiconductor material. The copper is present in an amount of 1 to 5 wt. % based on the total weight of the semiconductor material, and where the tin oxide is in the form of a tetragonal phase with a crystallite size of 15 to 25 nm.
Claims20
1:
- A semiconductor material, comprising:
- tin oxide;
- bismuth;
- and
- copper,
- wherein the tin oxide is doped with the bismuth and the copper,
- wherein the bismuth is present in an amount of 1 to 5 weight percent (wt. %) based on a total weight of the semiconductor material,
- wherein the copper is present in an amount of 1 to 5 wt. % based on the total weight of the semiconductor material, and
- wherein the tin oxide is in the form of a tetragonal phase with a crystallite size of 15-25 nm.
6 more elements
2:
- The semiconductor material of claim 1, wherein the bismuth is present in an amount of 2 to 4 wt. % based on a total weight of the semiconductor material.
3:
- The semiconductor material of claim 1, wherein the copper is present in an amount of 2 to 4 wt. % based on a total weight of the semiconductor material.
4:
- The semiconductor material of claim 1, wherein the semiconductor material has a crystallite size of 21 to 25 nm.
5:
- The semiconductor material of claim 1, wherein the semiconductor material has a unit cell volume of 71.95 to 72.05 Å3.
6:
- The semiconductor material of claim 1, wherein the semiconductor material has a band gap of 2.85 to 2.9 eV.
7:
- The semiconductor material of claim 1, wherein the semiconductor material has a dielectric constant of 3000 to 3500 at a frequency of 50 Hz.
8:
- The semiconductor material of claim 1, wherein the semiconductor material is made by a process, comprising:
- dissolving a tin salt and a copper salt in a first organic solvent to form a first solution;
- dissolving a bismuth salt in a second organic solvent to form a second solution;
- mixing the first solution and the second solution and adding a base to form a precipitate;
- calcinating the precipitate at a first temperature of 350 to 450° C. for 30 to 90 minutes;
- and
- calcinating the precipitate at a second temperature of 550 to 650° C. for 1 to 3 hours to form the semiconductor material.
4 more elements
9:
- A method of photocatalytic degradation, comprising:
- contacting the semiconductor material of claim 1 with a solution comprising one or more pollutants;
- irradiating the solution;
- and
- degrading the one or more pollutants in the solution.
2 more elements
10:
- The method of claim 9, wherein the one or more pollutants are selected from a group consisting of Congo red, imidacloprid, and malachite green.
11:
- The method of claim 9, wherein the irradiating occurs for 5 to 70 minutes.
12:
- The method of claim 9, wherein the semiconductor material has a photocatalytic efficiency of 90 to 99% based on an initial concentration of the one or more pollutants.
13:
- The method of claim 9, wherein the semiconductor material has an adsorption activity of 25 to 35% based on an initial concentration of the one or more pollutants.
14:
- The method of claim 10, wherein the one or more pollutants is Congo red and the semiconductor material has a photocatalytic efficiency of 96 to 98% based on an initial concentration of the Congo red.
15:
- The method of claim 10, wherein the one or more pollutants is imidacloprid and the semiconductor material has a photocatalytic efficiency of 92 to 94% based on an initial concentration of the imidacloprid.
16:
- The method of claim 10, wherein the one or more pollutants is malachite green and the semiconductor material has a photocatalytic efficiency of 97 to 99% based on an initial concentration of the malachite green.
17:
- The method of claim 11, wherein the irradiating occurs for 60 minutes and the semiconductor material has a chemical oxygen demand removal of 92 to 96%.
18:
- The method of claim 11, wherein the irradiating occurs for 60 minutes and the semiconductor material has a total organic carbon removal of 94 to 98%.
19:
- The method of claim 9, wherein hydroxyl radicals and superoxide anion radicals are involved in the degradation of the one or more pollutants.
20:
- The method of claim 9, further comprising:
- repeating the contacting and the irradiating 2 to 5 times,
- wherein the one or more pollutants in the solution are degraded by at least 85% based on an initial concentration of the one or more pollutants.