Method of obtaining insulating coating composition, coating composition and conductive materials comprising the same
AssigneeWeg Tintas Ltda
InventorsCristiane MEDEIROS, Priscila DA COSTA
Life of this patent
Estimating the term…
Abstract
A method of obtaining insulating coating material, coating composition and conductive materials comprising the same. In particular, a method of obtaining coating material comprising polyester and polyesterimide, without using cresol and derivatives as solvents. The formation of polyesterimide occurs in two steps—polyester formation followed by obtaining the imide moiety. Also the coating composition obtained by the present method and conductive material comprising the composition.
Claims25
A method of obtaining insulating coating composition comprising the steps of:
- i) carrying out a polyesterification reaction, by the forming isolated polyester in situ in a solid medium by loading the reaction medium with monomers of at least one acidic component, in a concentration range of 5% to 10%;
- monomers of at least one alcoholic component, in a range of 3% to 25%;
- and at least one catalyst, in a range of 0.01% to 1.0%, under heating from 180 to 260° C. until an acid number of less than 5 mgKOH/g is reached;
- ii) carrying out a polycondensation reaction comprising:
- a) forming an imide moiety in situ in a solid medium by loading the reaction medium with monomers of at least one acidic component, in a range of 8% to 18%;
- and monomers of at least one amine component, in a range of 2% to 10% under heating from 180 to 260° C., for 1 to 8 hours;
- b) cooling the medium to a temperature range between 12° and 180° C., with new loading of the reaction medium with monomers of at least one acidic component, in a range of 8% to 18%;
- and monomers of at least one amine component, in a range of 2% to 10%, until the medium reaches a kinematic viscosity in the range of 50 to 80 seconds;
- iii) dissolving the material resulting from step ii, using at least one organic solvent selected from the group consisting of glycol ethers, dimethylglycol, ethylglycol, isopropylglycol, butylglycol, methyldiglycol, ethyldiglycol, butyldiglycol, 3,5,5-trimethyl-2-cyclohexen-1-one, alkylbenzene, phenyl glycol, glycol ether esters, methyl glycol acetate, butyl glycol acetate, and methoxypropylacetate;
- iv) carrying out additivation by incorporating at least one additive at a temperature below 100° C. selected from the group consisting of a curing additive, chain-increasing additive and antioxidant additive;
- v) adjusting viscosity by adding an organic solvent, diluent or a combination thereof, at a temperature below 100° C.
8 more elements