Glass-ceramic sealing material
AssigneeNihon Yamamura Glass Co., Ltd.
InventorsKozo Maeda, Takuya Takayama
Life of this patent
Estimating the term…
Abstract
A crystallized glass composition not containing alkali metal oxides can be used at a temperature of 750° C. or lower by being fired at 650 to 750° C. The composition is a sealing glass composition substantially not containing alkali metal oxides, and containing, in mol %, SiO2: 8 to 20%, B2O3: 16 to 35%, BaO: 23 to 43%, ZnO: 0 to 26%, and CaO+SrO: 0 to 36%. The glass composition, when fired at a temperature of 700° C. in a form of a powder, forms a crystallized glass that exhibits a thermal expansion coefficient of 110 to 150×10−7/° C. at 50 to 700° C.
Claims10
A sealing glass composition substantially not comprising alkali metal oxides, and comprising, in mol %,
- 8 to 20% of SiO2,
- 16 to 35% of B2O3,
- 23 to 43% of BaO,
- 0 to 26% of ZnO, and
- 0 to 36% of CaO+SrO,
- wherein the glass composition, when fired at a temperature of 700° C. in a form of a powder, forms a crystallized glass that exhibits a thermal expansion coefficient of 110 to 150× 10−7/° C. at 50 to 700° C.
Dependencies are inferred from the claim text.