Ferritic stainless steel with improved formability and manufacturing method therefor
AssigneePosco
InventorsJieon Park, Jongsu Paek
Life of this patent
Estimating the term…
Abstract
The disclosed specification relates to a ferritic stainless steel with improved formability by controlling the average grain diameter through alloy components and manufacturing processes and to a method for manufacturing same. A ferritic stainless steel having improved formability, according to an embodiment, may comprise, in percentage by weight: C: 0.0005-0.02%; N: 0.005-0.02%; Si: 0.01-1.0%; Mn: 0.01-1.0%; P: 0.001-0.05%; Cr: 10.0-30.0%; Nb: 0.05-0.5%; Ti: 0.05-0.5%; and the remainder being Fe and inevitable impurities, wherein an Erichsen height may be 6-50 mm.
Claims7
A ferritic stainless steel with improved formability, comprising, in percent by weight (wt %), 0.0005 to 0.02% of carbon (C), 0.005 to 0.02% of nitrogen (N), 0.01 to 1.0% of silicon (Si), 0.01 to 1.0% of manganese (Mn), 0.001 to 0.05% of phosphorus (P), 10.0 to 30.0% of chromium (Cr), 0.05 to 0.5% of niobium (Nb), 0.05 to 0.5% of titanium (Ti), the remainder of Iron (Fe), and inevitable impurities, and having an Erichsen height of 6 to 50 mm.
A method for manufacturing a ferritic stainless steel with improved formability, the method comprising:
- preparing a slab comprising, in percent by weight (wt %), 0.0005 to 0.02% of carbon (C), 0.005 to 0.02% of nitrogen (N), 0.01 to 1.0% of silicon (Si), 0.01 to 1.0% of manganese (Mn), 0.001 to 0.05% of phosphorus (P), 10.0 to 30.0% of chromium (Cr), 0.05 to 0.5% of niobium (Nb), 0.05 to 0.5% of titanium (Ti), the remainder of Iron (Fe), and inevitable impurities, and having an Erichsen height of 6 to 50 mm;
- reheating the slab to 1100 to 1300° C. and then performing hot-rolling and hot-annealing on the reheated slab to produce a hot-rolled material;
- and
- performing cold-rolling and cold-annealing on the hot-rolled material, which has been subjected to the hot-annealing, two to five times to produce a steel plate,
- wherein the cold-annealing is performed at 850 to 1000° C.
Dependencies are inferred from the claim text.