Method for recovering polyester and method for manufacturing recycled polyester
AssigneeTeijin Frontier Co., Ltd.
InventorsRyo TSURUDA, Satoshi SUNOUCHI
Life of this patent
Estimating the term…
Abstract
A polyester which is less colored is obtained by treating a fiber product containing a polyester fiber and a Polyurethane fiber with an aromatic alcohol at a temperature in the range of from (the glass transition temperature of the polyester) to {(the glass transition temperature of the polyester)+100° C.}.
Claims10
A method for recovering a polyester, comprising treating a fiber product, which is comprised mainly of a fiber formed from a polyester, and which contains a fiber formed from a polymer having a urethane group as a constituent, with a solution of an aromatic alcohol or a derivative thereof at a temperature in the range of from (the glass transition temperature of the polyester) to {(the glass transition temperature of the polyester)+100° C.}.
Dependencies are inferred from the claim text.