Method of forming lithium-free glass articles having improved compressive stress and reduced warp
AssigneeCorning Incorporated
InventorsOzgur Gulbiten, Atul Kumar, Qiang Zhang, Zheming Zheng
Life of this patent
Estimating the term…
Loading patent…
AssigneeCorning Incorporated
InventorsOzgur Gulbiten, Atul Kumar, Qiang Zhang, Zheming Zheng
Estimating the term…
A method of forming a lithium-free glass article includes thermally treating the glass article to impart a fictive temperature and ion exchanging the thermally treated glass article. The thermal treatment includes heating the glass article to a hold temperature from 130° C. below to 20° C. above an annealing point of the glass article; holding the glass article at the hold temperature for a hold period; cooling the glass article at a first cooling rate from the hold temperature to an intermediate temperature; and cooling the glass article at a second cooling rate from the intermediate temperature to room temperature. The ion exchanged glass article includes a compressive stress greater than or equal to 900 MPa, as measured for an article having a thickness of 1.1 mm; and a warp less than or equal to 0.3 mm, as measured for an article having a length less than 200 mm.
A method of forming a lithium-free glass article, the method comprising:
Dependencies are inferred from the claim text.