Soft thermoplastic elastomer powder material and preparation method thereof
AssigneeIndustrial Technology Research Institute
InventorsJin-An WU, Chen-Yu LIU, Chin-Lang WU
Life of this patent
Estimating the term…
Loading patent…
AssigneeIndustrial Technology Research Institute
InventorsJin-An WU, Chen-Yu LIU, Chin-Lang WU
Estimating the term…
A soft thermoplastic elastomer powder has a thermal conductivity coefficient of 0.25 to 0.45 W/mK, a Shore hardness of 20D to 49D, a process window of ≥20° C., and a melt viscosity of less than 1,000 Pa*s (0.63 rad/s) at a specific temperature (Tm+30° C.). The soft thermoplastic elastomer powder includes 100 parts by weight of a thermoplastic polyurethane elastomer, 0.01 to 2.0 parts by weight of a thermal conductive agent, and 0.05 to 2.0 parts by weight of a flow aid agent. The process window of the thermoplastic polyurethane elastomer is ≥15° C. The thermal conductivity coefficient of the thermal conductive agent is 50 to 400 W/mK, and the particle size of the thermal conductive agent is 0.5 μm to 6 μm.
A soft thermoplastic elastomer powder, comprising:
A preparation method of a soft thermoplastic elastomer powder, comprising:
Dependencies are inferred from the claim text.