Described herein is a polyolefin composite and a method of preparation. The method includes blending a mixture comprising 50 to 94.9 weight percent (wt %) of a matrix polymer, 5 to 40 wt % of a reinforcement polymer; and 1 to 20 wt % of a crosslinked molecule and/or 0.1 to 10 wt % of a nanofiller to provide a blended mixture, wherein the weight percent of each component is with respect to the polyolefin composite; and forming the polyolefin composite from the blended mixture, wherein the matrix polymer is a first polyolefin with a number average molecular weight of at most 300,000, and the reinforcement polymer is a second polyolefin with a number average molecular weight of at least 1,500,000. The polyolefin composite includes the matrix polymer, the reinforcement polymer, and the crosslinked molecule and/or the nanofiller as described aforementioned.
-34. (canceled)
A method of preparing a polyolefin composite, the method comprising:
A polyolefin composite consisting essentially of 50 to 94.9 wt % of high density polyethylene, 5 to 40 wt % of ultra-high molecular weight polyethylene, and 1 to 20 wt % of crosslinked ethylene having a degree of crosslinking of 10% or less, wherein the high density polyethylene has a number average molecular weight of at most 300,000, the ultra-high molecular weight polyethylene has a number average molecular weight of at least 1,500,000.