Back to results
US 2026/0151756 A1Published application
Method for preparing catalyst using recycled waste batteries and application of the catalyst
AssigneeGuizhou Normal University
InventorsWei Gong, Mo Liu, Yang Dai, Zhen Yao
Life of this patent
Estimating the term…
Abstract
Provided herein is a method for preparing a catalyst form recycled waste batteries, which includes the preparation of a NiCoMnOx composite oxide, and further extends to the preparation of a perovskite catalyst and a core-shell loaded noble catalyst.
Claims10
A catalyst prepared from recycled waste batteries, comprising:
- a shell structure,
- a core structure prepared from valuable components of waste ternary lithium power batteries, and
- a gap layer between the core structure and the shell structure,
- wherein the core structure is composed of a composite metal oxide consisting of NiO, Co3O4 and MnO2,
- wherein the shell structure is a manganese dioxide layer covering a surface of the core structure, and the manganese dioxide layer is provided with at least two through-channels,
- wherein noble metals Pt and/or Ru are loaded on an outer surface of the manganese dioxide layer and inside the gap layer.
3 more elements
A method for preparing a catalyst form recycled waste batteries, comprising:
- extracting valuable metals from cathode materials of waste ternary power batteries with an inorganic acid to form Ni, Co, and Mn precursor salts, wherein the inorganic acid is selected from the group consisting of H2SO4, HNO3 and HCl;
- adding a precipitant to the precursor salts to generate a composite metal precipitate, wherein the precipitant is selected from the group consisting of Na2CO3, saturated NH4(NO3)2, NH3·H2O and NaOH;
- calcining the composite metal precipitate to prepare a NiCoMnOx composite metal oxide containing NiO, Co3O4 and MnO2;
- pulverizing the composite metal oxide to a particle size of 200 μm-250 μm to obtain a powder of the composite metal oxide, uniformly dispersing polymethyl methacrylate microspheres, manganese dioxide particles and α-hemihydrate gypsum in anhydrous ethanol to obtain a mixed material, spraying the mixed material on a surface of the powder of the composite metal oxide, and drying to form a mixed material layer on the surface of the powder of the composite metal oxide to obtain a composite intermediate;
- adding 0.3 g-1.2 g of potassium permanganate into 20 g-25 g of 0.2 mol/L sodium hydroxide solution to obtain an alkaline potassium permanganate solution;
- dispersing the composite intermediate in the anhydrous ethanol, then adding 0.2 mol/L sodium hydroxide solution, and stirring to form a suspension, wherein a mass ratio of the composite intermediate, the anhydrous ethanol, and the sodium hydroxide solution is 1:(80-100):(2.5-5);
- dropping slowly the alkaline potassium permanganate solution into the suspension, wherein the volume ratio of the suspension to the alkaline potassium permanganate solution is 100:(5-10), then stirring them and allowing the reaction to proceed for 300 minutes, filtering out a first solid after the reaction, repeatedly washing the first solid with deionized water, and then drying at 80° C. to obtain composite microspheres;
- adding the composite microspheres into deionized water, dissolving α-hemihydrate gypsum, filtering out a second solid, washing the second solid with deionized water to obtain a catalyst microsphere intermediate I, calcining the catalyst microsphere intermediate I at 280° C. for 2 to 3 hours, then cooling, and then adding deionized water for ultrasonic washing and drying to obtain a catalyst microsphere intermediate II;
- immersing the catalyst microsphere intermediate II in a noble metal precursor solution, filtering out a third solid, then drying and grinding the third solid and placing them it into a tube furnace, and then introducing a 10% H2/Ar gas mixture and maintaining at 400° C. for 4 hours to obtain a core-shell loaded noble metal catalyst.
6 more elements
Dependencies are inferred from the claim text.