Methods for reduction of photoresist defect
AssigneeTaiwan Semiconductor Manufacturing Company, Ltd.
InventorsChun-Wei LIAO, Hui-Chun LEE
Life of this patent
Estimating the term…
Abstract
The present disclosure in various embodiments provides a hardened resist layer that can reduce resist scum defects in a resist layer. In one embodiment, a lithography method is provided. The method includes forming a resist layer over a substrate, performing an exposure process on the resist layer, performing a developing process on the resist layer to form a patterned resist layer having a plurality resist segments, exposing the patterned resist layer to a vacuum ultraviolet (VUV) radiation, and subjecting the resist pattern to a de-scum process.
Claims20
A lithography method, comprising:
- forming a resist layer over a substrate;
- performing an exposure process on the resist layer;
- performing a developing process on the resist layer to form a patterned resist layer having a plurality resist segments and a resist scum protruding from sidewalls of the resist segments and extending between two adjacent resist segments, wherein the resist scum is exposed to an exposure light at the exposure process;
- hardening the patterned resist layer including the resist scum by exposing the patterned resist layer to a vacuum ultraviolet (VUV) radiation;
- and
- after exposing the patterned resist layer to the VUV radiation, subjecting the resist pattern to a de-scum process that is substantially free of VUV radiation to remove the resist scum.
A lithography method, comprising:
- performing an exposure process on a resist layer over a substrate;
- performing a developing process on the resist layer to form a patterned resist layer having a plurality resist segments and a resist scum protruding from sidewalls of the resist segments and extending between two adjacent resist segments, wherein the resist scum is exposed to an exposure light at the exposure process, and wherein each resist segment has a first critical dimension after the developing process;
- hardening the patterned resist layer by exposing the patterned resist layer to a photon radiation, wherein each resist segment has a second critical dimension after exposing the patterned resist layer to the photon radiation, and the second critical dimension is smaller than the first critical dimension;
- after exposing the patterned resist layer to the photon radiation, bombarding the patterned resist layer with energetic particles in an environment that is substantially free of VUV light to remove the resist scum, wherein each resist segment has a third critical dimension after the bombardment process, and the third critical dimension is smaller than the second critical dimension;
- and
- performing an etching process on the patterned resist layer.
A lithography method, comprising:
- performing an exposure process on a resist layer over a substrate;
- forming a patterned resist layer, wherein the patterned resist layer has a plurality resist segments and a resist scum protruding from sidewalls of the resist segments and extending between two adjacent resist segments, wherein the resist scum is exposed to an exposure light at the exposure process;
- hardening the patterned resist layer in a vacuum chamber by exposing the patterned resist layer to a vacuum ultraviolet (VUV) light, wherein the VUV light maintains the resist scum, and the patterned resist layer has a reduced critical dimension after the VUV exposure;
- after hardening the patterned resist layer, performing an ion bombardment process on the patterned resist layer in an environment that is substantially free of VUV light to remove the resist scum;
- and
- performing an etching process directed to remove a material layer disposed below the patterned resist layer, wherein the material layer is etched using the patterned resist layer as a mask.
Dependencies are inferred from the claim text.