Back to results
US 2026/0138925 A1Published application
Lead-zinc tailings-based ceramsite
AssigneeHenan Building Materials Research and Design Institute Co., Ltd.
InventorsMaoliang Zhang, Xindi Wan, Yan Ma, Jianwei Li, Jinhua Wang, Lu Zhang, Huanhuan Zhang, Huiling Yin
Life of this patent
Estimating the term…
Abstract
A lead-zinc tailings-based ceramsite includes the following raw materials in parts by mass: 100 parts of lead-zinc tailings; 20-30 parts of limestone tailings; 6-8 parts of activated mullite nanopowder, 1-3 parts of glass powder, and 8-12 parts of dried sludge powder. A preparation method for the lead-zinc tailings-based ceramsite is further provided.
Claims8
A lead-zinc tailings-based ceramsite, comprising the following raw materials in parts by mass:
- 100 parts of lead-zinc tailings;
- 20-30 parts of limestone tailings;
- 6-8 parts of activated mullite nanopowder;
- 1-3 parts of glass powder;
- and
- 8-12 parts of dried sludge powder;
- wherein the activated mullite nanopowder is produced by uniformly dispersing mullite particles in a mixed solution of sodium silicate and potassium silicate, followed by heating and grinding, with a target temperature of 300-600° C.;
- and
- the lead-zinc tailings-based ceramsite is prepared according to following preparation method:
- (1) uniformly mixing the raw materials comprising the lead-zinc tailings, the limestone tailings, the activated mullite nanopowder, the glass powder, and the dried sludge powder in parts by mass, and adding water to prepare a ceramsite green body;
- (2) heating the ceramsite green body to temperature of 900-980° C. and maintaining the temperature for 5-8 min;
- and heating the ceramsite green body to temperature of 1200-1300° C. and maintaining the temperature for 8-10 min;
- and
- (3) cooling the ceramsite green body to temperature of 1150-1100° C. and maintaining the temperature for 5-10 min;
- cooling the ceramsite green body to temperature of 1080-1000° C. and maintaining the temperature for 5-10 min;
- cooling the ceramsite green body to temperature of 950-900° C. and maintaining the temperature for 5-10 min;
- and slowly cooling the ceramsite green body to standard ambient temperature to obtain the lead-zinc tailings-based ceramsite.
14 more elements