Base-mediated deconstruction of epoxy resins
AssigneeAarhus Universitet
InventorsHongwei Sun, Alexander Ahrens, Troels Skrydstrup
Life of this patent
Estimating the term…
Abstract
The present invention relates to a method for disassembly of epoxy-based polymers, the method comprising chemical manipulations to a cured epoxy resins involving a mixture of at least one organic solvent and a base. Specifically, the epoxy-based polymer is an amine-cured epoxy resin and the base is a nucleophilic base. The present invention allows for recycling of the constituents comprised in the cured epoxy resin in high yields, notably even in the absence of any metal catalyst.
Claims53
A method for the deconvolution of epoxy-based polymers (EBPs), the method comprising the steps:
- a. providing an EBP,
- b. contacting the EBP with a solvent system comprising at least one aprotic apolar organic solvent and an oxygen-containing base to form a suspension, and
- c. heating said suspension to a temperature of at least 130° C. for at least 2 hours, thereby releasing monomers of the EBPs into the suspension,
- wherein the base is added in an amount corresponding to from 20% to 100% by weight of the EBP, and wherein the method does not comprise or make use of a catalyst.
The method according to the preceding claim, wherein the EBP is derived from a bisphenol diglycidyl ether.
The method according to any one of the preceding claims, wherein the EBPs comprise the chemical motif of Formula (III-a)
- wherein,
- X1 is selected from the group consisting of H, R, or —C(═O)R, wherein R can be C1-6 alkyl, C1-6 heteroalkyl, C1-6 alkoxy, C1-6 allyl, C1-6 heteroallyl, C4-8 cycloalkyl, C4-8 heterocycloalkyl, C4-8 aryl, and C4-8 heteroaryl, each of which may be optionally substituted with one or more of —OH, —NH2, -L, -CL3, —OCH3, wherein L is a halogen;
- X2 is selected from the group consisting of C4-8 cycloalkyl, C4-8 heterocycloalkyl, C4-8 aryl, and C4-8 heteroaryl, each of which may be optionally substituted with one or more of —OH, —NH2, -Q, -CQ3, —OCH3, wherein each of Q is independently hydrogen, halogen, methyl, phenyl or benzyl;
- and
- n represents the motif as repeating, and may be an integer larger than 1.
The method according to any one of the preceding claims, wherein the EBP is an amine-cured epoxy resin.
The method according to any one of the preceding claims, wherein the EBPs comprise the chemical motif of Formula (III-a(i)):
- wherein,
- X1 is selected from the group consisting of H, R, or —C(═O)R,
- X2 is selected from the group consisting of C4-8 cycloalkyl, C4-8 heterocycloalkyl, C4-8 aryl, and C4-8 heteroaryl, each of which may be optionally substituted with one or more of —OH, —NH2, -Q, -CQ3, —OCH3, wherein each of Q is independently hydrogen, halogen, methyl, phenyl or benzyl,
- X3 is selected from the group consisting of CR2, NZ, O, and S,
- wherein R can be C1-6 alkyl, C1-6 heteroalkyl, C1-6 alkoxy, C1-6 allyl, C1-6 heteroallyl, C4-8 cycloalkyl, C4-8 heterocycloalkyl, C4-8 aryl, and C4-8 heteroaryl, each of which may be optionally substituted with one or more of —OH, —NH2, -L, -CL3, —OCH3, wherein L is a halogen,
- wherein NZ represents an amine based crosslinker and/or hardener selected from the group consisting of poly amide resins, poly(oxypropylene)diamine, 3-aminomethyl-3,5,5-trimethylcyclohexylamine, triethylenetetramines, tetraethylene-pentamines, and trimethylolpropane tris[poly(propylene glycol), amine terminated]ether (T-403), and
- wherein n represents the motif as repeating, and may be an integer larger than 1.
The method according to any one of the preceding claims, wherein the EBPs comprise the chemical motif of formula (III-da):
- wherein R5 is selected as O or NZ, wherein NZ represents an amine based crosslinker and/or hardener selected from the group consisting of poly amide resins, poly(oxypropylene)diamine, 3-aminomethyl-3,5,5-trimethylcyclohexylamine, triethylenetetramines, tetraethylene-pentamines, and trimethylolpropane tris[poly(propylene glycol), amine terminated]ether (T-403), and wherein Ar represent an aromatic ring such as phenyl or naphthyl, preferably phenyl.
The method according to any one of the preceding claims, wherein the EBPs are bisphenol based EBPs, such as bisphenol A-based EBPs.
The method according to any one of the preceding claims, wherein the monomers released into the suspension are bisphenol-based monomers.
The method according to any one of the preceding claims, wherein the monomers released into the suspension are bisphenol A-based monomers.
The method according to any one of the preceding claims, wherein the monomers released into the suspension are bisphenol A.
The method according to any one of the preceding claims, wherein the method allows for direct separation and isolation of bisphenol A-based monomers.
The method according to any one of the preceding claims, wherein the EBPs comprise the chemical motif of formula (III-ca):
- wherein the motif of Formula (III-ca) may comprise from 1 to 4 of each of R3 and R4, and wherein R1, R2, R3, and R4 are each individually selected from the group consisting of H, C1-6 alkyl, C1-6 alkenyl, CF3, F, Cl, Br, OH, NO2, NH2, phenyl, or wherein R1 and R2 may come together to form a C6-cycloalkyl, and wherein R5 is selected as O or NZ, wherein NZ represents an amine based crosslinker and/or hardener selected from the group consisting of poly amide resins, poly(oxypropylene)diamine, 3-aminomethyl-3,5,5-trimethylcyclohexylamine, triethylenetetramines, tetraethylene-pentamines, and trimethylolpropane tris[poly(propylene glycol), amine terminated]ether (T-403).
The method according to any one of the preceding claims, wherein the suspension is heated to a temperature between 130° C. to 250° C.
The method according to any one of the preceding claims, wherein the suspension is heated to a temperature between 170° C. and 250° C.
The method according to any one of the preceding claims, wherein the suspension is heated to a temperature between 170° C. and 210° C.
The method according to any one of the preceding claims, wherein the suspension is heated for at least 2 hours, such as for at least 4 hours, such as for at least 8 hours, such as for at least 16 hours, such as for at least 24 hours.
The method according to any one of the preceding claims, wherein the suspension is heated for a time ranging from 2 hours to 10 days, such as from 2 hours to 4 hours, such as from 4 hours to 8 hours, such as from 8 hours to 16 hours, such as from 16 hours to 24 hours, such as from 24 hours to 2 days, such as from 2 days to 3 days, such as from 3 days to 5 days, such as from 5 days to 10 days.
The method according to any one of the preceding claims, wherein the organic solvent is selected from the group consisting of toluene, benzene, xylene, mesitylene, cumene, cymene, and xylol, or a structural isomer of any one of these.
The method according to any one of the preceding claims, wherein the organic solvent is selected from the group consisting of toluene, xylene and cymene, or a structural isomer of any one of these.
The method according to any one of the preceding claims, wherein the organic solvent is selected from the group consisting of toluene, p-cymene, o-xylene.
The method according to any one of the preceding claims, wherein the oxygen-containing base is a hydroxide selected from the group consisting of NaOH, LiOH, KOH, CsOH, RbOH, Ca(OH)2, Sr(OH)2, and Ba(OH)2;
- or an alkoxide selected from the group consisting of n-butoxide, tert-butoxide, methoxide, ethoxides, and isopropoxide, including sodium or potassium salts of these.
The method according to any one of the preceding claims, wherein the base is selected from the group consisting of NaOH, KOH, NaOBu, and NaOtBu.
The method according to any one of the preceding claims, wherein the base is a nucleophile base.
The method according to any one of the preceding claims, wherein the base is not a nitrogen-containing base.
The method according to any one of the preceding claims, wherein the method is conducted in a closed vessel under autogenous pressure.
The method according to any one of the preceding claims, wherein the method is performed in a closed vessel under an autogenous pressure of 14.5 to 145 psi.
The method according to any one of the preceding claims, wherein the method is performed in an inert atmosphere, such as an atmosphere consisting essentially of nitrogen (N2) or Argon (Ar).
The method according to any one of the preceding claims, wherein the method is a one pot reaction.
The method according to any one of the preceding claims, wherein the epoxy-based polymer may be mixed with fibres, such as in fibre-reinforced composites, in particular those where the fibres are glass fibre or carbon fibre.
The method according to any one of the preceding claims, wherein the EBP is a powder.
The method according to any one of the preceding claims, wherein the method does not comprise or make use of hydrogen peroxide.
The method according to any one of the preceding claims, wherein the method does not comprise or make use of ascorbic acid.
The method according to any one of the preceding claims, wherein the method does not comprise or make use of either of hydrogen peroxide or ascorbic acid.
The method according to any one of the preceding claims, wherein the EBPs have not been chemically treated prior to the step of contacting said EBPs with the suspension comprising at least one aprotic apolar organic solvent and an oxygen-containing base.
The method according to any one of the preceding claims, wherein the steps a, b, and c are performed sequentially in the specified order.
Dependencies are inferred from the claim text.