Method for recovering nickel hydroxide and nickel sulfate from nickel-containing materials
AssigneeKorea Institute of Geoscience and Mineral Resources
InventorsTae-Gong RYU, Jun-Ho SHIN, Jae-Min JEONG
Life of this patent
Estimating the term…
Abstract
The present invention provides a method for recovering nickel hydroxide and nickel sulfate from nickel-containing materials, wherein the nickel-containing materials are crushed and pulverized and then leached with sulfuric acid, leached residue separation and filtrate separation are performed and then the pH is adjusted to recover nickel hydroxide, and the recovered nickel hydroxide is further subjected to a sulfation reaction to recover nickel sulfate.
Claims15
A method for recovering nickel hydroxide from nickel-containing material, comprising steps of:
- (a-1) crushing and pulverizing a multilayer ceramic capacitor process sludge;
- (a-2) leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate;
- (a-3) separating a leached residue and the primary filtrate from the first sulfuric acid leachate;
- (a-4) performing a primary pH adjustment on the first sulfuric acid leachate, from which the leached residue has been separated, to form a second sulfuric acid leachate containing a primary pH-adjusted impurity precipitate and a secondary filtrate;
- (a-5) separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate;
- (a-6) performing a secondary pH adjustment on the second sulfuric acid leachate, from which the impurity precipitate has been separated, to separate nickel hydroxide;
- and
- (a-7) washing the separated nickel hydroxide to recover nickel hydroxide, wherein in the step (a-2) of leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate,
- a leaching temperature ranges from 10 to 90° C.
A method for recovering nickel sulfate from nickel-containing material, comprising steps of:
- (a-1) crushing and pulverizing a multilayer ceramic capacitor process sludge;
- (a-2) leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate;
- (a-3) separating a leached residue and the primary filtrate from the first sulfuric acid leachate;
- (a-4) performing a primary pH adjustment on the first sulfuric acid leachate, from which the leached residue has been separated, to form a second sulfuric acid leachate containing a primary pH-adjusted impurity precipitate and a secondary filtrate;
- (a-5) separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate;
- (a-6) performing a secondary pH adjustment on the second sulfuric acid leachate, from which the impurity precipitate has been separated, to separate nickel hydroxide;
- (a-7) washing the separated nickel hydroxide to recover nickel hydroxide;
- and
- (a-8) performing a sulfation reaction between the recovered nickel hydroxide and a sulfuric acid compound to recover nickel sulfate,
- wherein in the step (a-2) of leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate,
- a leaching temperature ranges from 10 to 90° C.
Dependencies are inferred from the claim text.