R-t-b based permanent magnet and method of manufacturing the same
AssigneeTDK Corporation
InventorsKoji MIURA, Hiroki KAWAMURA
Life of this patent
Estimating the term…
Abstract
An R-T-B based permanent magnet contains 28.0 mass % or more and 31.5 mass % or less light rare earth element in total, more than 0 mass % and 1.0 mass % or less heavy rare earth element in total, 0.97 mass % or more and 1.05 mass % or less B, 0.05 mass % or more and 0.52 mass % or less Al, 0.50 mass % or more and 0.75 mass % or less Zr, 0 mass % or more and 0.20 mass % or less Ga, and 0 mass ppm or more and 1000 mass ppm or less O. The R-T-B based permanent magnet has a coercivity of 715 kA/m or more at 160° C.
Claims7
An R-T-B based permanent magnet comprising:
- 28.0 mass % or more and 31.5 mass % or less light rare earth element in total;
- more than 0 mass % and 1.0 mass % or less heavy rare earth element in total;
- 0.97 mass % or more and 1.05 mass % or less B;
- 0.05 mass % or more and 0.52 mass % or less Al;
- 0.50 mass % or more and 0.75 mass % or less Zr;
- 0 mass % or more and 0.20 mass % or less Ga;
- and
- 0 mass ppm or more and 1000 mass ppm or less O,
- wherein the R-T-B based permanent magnet has a coercivity of 715 kA/m or more at 160° C.
A method of manufacturing an R-T-B based permanent magnet, comprising:
- preparing a main alloy and a sub alloy;
- and
- mixing the main alloy and the sub alloy,
- wherein
- the main alloy comprises 1.03 mass % or more and 1.11 mass % or less B, and
- the sub alloy comprises 0.96 mass % or more and 15.0 mass % or less Zr.
Dependencies are inferred from the claim text.