Method for carbonizing a polymeric object in a molten medium
OwnerFelix L. Paulauskas, Hippolyte Grappe +1inventors
InventorsFelix L. Paulauskas, Hippolyte Grappe, Joshua Nowak
Life of this patent
Estimating the term…
Loading patent…
OwnerFelix L. Paulauskas, Hippolyte Grappe +1inventors
InventorsFelix L. Paulauskas, Hippolyte Grappe, Joshua Nowak
Estimating the term…
A method for producing a carbonized object, the method comprising immersing a partially carbonized polymeric object into a molten anhydrous medium maintained within a temperature range of 300° C.-1800° C. for a period of time of 0.25-30 minutes under an inert atmosphere to result in conversion of the partially carbonized object into the carbonized object, wherein said partially carbonized polymeric object is 30-70 wt % carbon and the carbonized object is at least 90 wt % carbon. Also described herein is an apparatus useful in practicing the above described method, wherein the apparatus includes a vessel (crucible) constructed of a thermally refractory material for holding the molten medium, and a lid that contains one or more protruding elements (i.e., prongs or projections) or rollers useful for maintaining a polymeric fiber or ribbon immersed in the molten medium.
A method for producing a carbonized object, the method comprising immersing a partially carbonized polymeric object into a molten anhydrous medium maintained within a temperature range of 300° C.-1800° C. for a period of time of 0.25-30 minutes under an inert atmosphere to result in conversion of the partially carbonized object into the carbonized object, wherein said partially carbonized polymeric object is 30-70 wt % carbon and the carbonized object is at least 90 wt % carbon.
An apparatus useful in immersing a carbonizable continuous fiber or ribbon in a high temperature molten medium, the apparatus comprising:
Dependencies are inferred from the claim text.