Cathode material, and battery
AssigneeBtr (Jiangsu) New Material Technology Co., Ltd
InventorsYU WANG, Shuxian HUANG, Xiong SONG, Yu ZHENG, Pingzhou YANG, Shunyi YANG
Life of this patent
Estimating the term…
Loading patent…
AssigneeBtr (Jiangsu) New Material Technology Co., Ltd
InventorsYU WANG, Shuxian HUANG, Xiong SONG, Yu ZHENG, Pingzhou YANG, Shunyi YANG
Estimating the term…
A cathode material, a preparation method thereof, and a battery provided. The cathode material is a nickel-lithium cobalt oxide based composite oxide including a core and a surface reconstruction layer arranged outside the core, where the surface reconstruction layer is a region etched away by dissolving the cathode material with 100 times diluted aqua regia for 30 minutes, with an ambient temperature controlled to be 300° C. during dissolution, and the core is a remaining region after the surface reconstruction layer is etched away from the cathode material, and where the core has a Li molar content of m1, the surface reconstruction layer has a Li molar content of m2, and 1.3≤m2/m1≤4.0. The cathode material provided is improved stability of crystal structure while having high capacity, thereby improving cycle stability of the cathode material and improving withstand voltage of the cathode material.
A cathode material, wherein the cathode material is a nickel-lithium cobalt oxide based composite oxide comprising a core and a surface reconstruction layer arranged outside the core, wherein the surface reconstruction layer is a region etched away by dissolving 0.3 g of the cathode material with 100 times diluted 0.4 ml of aqua regia for 30 minutes, with an ambient temperature controlled to be 300° C. during dissolution, and the core is a remaining region after the surface reconstruction layer is etched away from the cathode material, and wherein the core has a Li molar content of m1, the surface reconstruction layer has a Li molar content of m2, and 1.3≤m2/m1≤4.0.
A cathode material, wherein the cathode material is a nickel-lithium cobalt oxide based composite oxide comprising a core and a surface reconstruction layer arranged outside the core, wherein the surface reconstruction layer is a region etched away by dissolving 0.3 g of the cathode material with 100 times diluted 0.4 ml of aqua regia for 30 minutes, with an ambient temperature controlled to be 300° C. during dissolution, and the core is a remaining region after the surface reconstruction layer is etched away from the cathode material, and wherein the surface reconstruction layer has a Li molar content of m2, the cathode material has a total Li molar content of mLi total, and 1.1≤m2/mLi total≤3.0.
Dependencies are inferred from the claim text.