High-strength lithium ion battery diaphragm and preparation method thereof
AssigneesChangzhou Senior New Energy Material Co., Ltd., Shenzhen Senior Technology Material Co., Ltd.
InventorsChuang LI, Wuhua XIAO, Jinbo WANG, Yaqiang CUI, Chen GUO
Life of this patent
Estimating the term…
Abstract
Some embodiments relate to the technical field of lithium ion battery diaphragms. Provided are an ultrathin lithium ion battery diaphragm with high mechanical strength and excellent thermal dimensional stability, and a preparation method thereof.
Claims20
A lithium-ion battery separator, comprising a core layer and surface layers covering upper and lower surfaces of the core layer, wherein the core layer has porousness and the surface layers have porousness, and the core layer and the surface layers satisfy at least one of following two conditions:
- 1) a weight-average molecular weight of the core-layer polymer being 1.1 million-1.7 million, preferably 1.2 million-1.7 million, more preferably 1.3 million-1.6 million, and further preferably 1.4 million-1.55 million, wherein the weight-average molecular weight of the core-layer polymer is 1.01-2.20 times a weight-average molecular weight of the surface-layer polymer, preferably 1.05-1.80 times, and further preferably 1.10-1.30 times;
- and
- 2) a melt index of the surface-layer polymer being 1.01-2.00 times a melt index of the core-layer polymer, preferably 1.05-1.70 times, and further preferably 1.10-1.50 times, wherein the melt index is measured at 190° C., 2.16 kg/10 min.
A lithium-ion battery separator, wherein in a direction from separator surfaces of two sides respectively to a center of the separator, a porous separator layer A polymer, comprising 2.5˜10%, preferably 4.5-9%, and further preferably 6-7.5% of a separator layer thickness, has a weight-average molecular weight a or a melt index a′;
- and a porous separator layer B polymer, comprising a remaining central part, has a weight-average molecular weight b or a melt index b′, which satisfies at least one of following two conditions:
- 1) the weight-average molecular weight b being 1.1-1.7 million, preferably 1.2-1.7 million, more preferably 1.3 million-1.6 million, and further preferably 1.4 million-1.55 million, wherein the weight-average molecular weight b is 1.01-2.20 times the weight-average molecular weight a, preferably 1.05-1.80 times, and further preferably 1.10-1.30 times;
- and
- 2) the melt index a′ being 1.01-2.00 times the melt index b′, preferably 1.05-1.70 times, and further preferably 1.10-1.50 times, wherein the melt index is measured at 190° C., 2.16 kg/10 min.
A manufacturing method for a lithium-ion battery separator, comprising following steps:
- 1) preparing a material of surface layer and a material of core layer;
- 2) melting and molding the material of surface layer to be a surface layer, and melting and molding the material of core layer to be a core layer, wherein the surface layer covers upper and lower surfaces of the core layer to form a stacked layer body;
- 3) bi-directionally stretching the stretched stacked layer body to obtain a stretched stacked layer body;
- 4) removing a pore-forming agent from the stretched stacked layer body to obtain a separator precursor;
- and
- 5) performing heat setting on the separator precursor to obtain the lithium-ion battery separator, wherein
- the material of surface layer comprises a first polymer and the pore-forming agent, wherein the first polyethylene comprises a first polyethylene with a weight-average molecular weight of 300,000-600,000, preferably 400,000-550,000, and a second polyethylene with a weight-average molecular weight of 1.3 million-3.0 million, preferably 1.3 million-1.8 million;
- and a weight ratio of the first polyethylene to the second polyethylene is 0-80:20-100, preferably 1-50:50-99, more preferably 0-40:60-100, and most preferably 15-35:65-85;
- the material of core layer comprises a second polymer and the pore-forming agent, wherein the second polymer comprises a third polyethylene with a weight-average molecular weight of 300,000-600,000, preferably 400,000-550,000, and a fourth polyethylene with a weight-average molecular weight of 1.3 million-3.0 million, preferably 1.5 million-2.0 million, wherein a weight ratio of the third polyethylene to the fourth polyethylene is 0-30:70-100, preferably 1-10:90-99, and more preferably 5-20:80-95;
- and
- the second polymer optionally comprises a fifth polypropylene with a weight-average molecular weight of 300,000-600,000, preferably 400,000-550,000, and the fifth polypropylene accounts for 0-20% of a weight of the second polymer, preferably 0˜13%.