Back to results
US 2026/0085391 A1Published application
Hot rolled steel sheet
AssigneeNippon Steel Corporation
InventorTakashi SHIMADA
Life of this patent
Estimating the term…
Abstract
Provided is a hot rolled steel sheet having a predetermined chemical composition, and a microstructure comprising, by area ratio, ferrite: 60 to 80%, bainite: 15 to 30%, and martensite: 3 to 10%, wherein TiC precipitates having a diameter of 1.0 to 5.0 nm are present in the ferrite in a number density of 1.0×1016 to 100.0×1016/cm3, and the hot rolled steel sheet has a tensile strength of 780 MPa or more tensile strength.
Claims2
A hot rolled steel sheet having a chemical composition comprising, by mass %,
- C:
- 0.010 to 0.100%,
- Si:
- 0.01 to 0.10%,
- Mn:
- 0.50 to 3.00%,
- Ti:
- 0.050 to 0.200%,
- Nb:
- 0.010 to 0.020%,
- Al:
- 0.100 to 1.000%,
- P:
- 0.1000% or less,
- S:
- 0.0100% or less,
- N:
- 0.0100% or less,
- O:
- 0.0100% or less,
- Ni:
- 0 to 2.000%,
- Mo:
- 0 to 1.000%,
- Cr:
- 0 to 2.000%,
- B:
- 0 to 0.0100%,
- Co:
- 0 to 2.000%,
- V:
- 0 to 1.000%,
- Cu:
- 0 to 2.000%,
- W:
- 0 to 1.0000%,
- Ta:
- 0 to 1.0000%,
- Sn:
- 0 to 1.0000%,
- Sb:
- 0 to 1.0000%,
- As:
- 0 to 0.0100%,
- Mg:
- 0 to 0.0100%,
- Ca:
- 0 to 0.0100%,
- Zr:
- 0 to 0.0100%,
- Hf:
- 0 to 0.0100%,
- Bi:
- 0 to 0.0100%,
- REM:
- 0 to 0.0100%, and
- balance:
- Fe and impurities, and
- a microstructure comprising, by area ratio,
- ferrite:
- 60 to 80%,
- bainite:
- 15 to 30%, and
- martensite:
- 3 to 10%, wherein
- TiC precipitates having a diameter of 1.0 to 5.0 nm are present in the ferrite in a number density of 1.0×1016 to 100.0×1016/cm3, and
- the hot rolled steel sheet has a tensile strength of 780 MPa or more.
64 more elements
Dependencies are inferred from the claim text.