Abstract
Described herein are compositions, and more particularly to alloy compositions, methods of using the alloy compositions, and articles formed from with the alloy compositions. The alloy compositions are broadly applicable in applications requiring superalloys, including welding processes, additive manufacturing processes, metal casting processes, coating processes, repairing processes, powder metallurgy, and/or combinations thereof.
Claims20
A composition comprising:
- from about 0.2 wt % to about 0.7 wt % hafnium;
- from about 4.0 wt % to about 5.5 wt % tantalum;
- from about 8 wt % to about 10 wt % tungsten;
- from about 0.06 wt % to about 0.1 wt % carbon;
- from about 9 wt % to about 10 wt % cobalt;
- from about 8 wt % to about 8.7 wt % chromium;
- from about 5.25 wt % to about 5.75 wt % aluminum;
- from about 0.5 wt % to about 1.5 wt % titanium;
- from about 0.4 wt % to about 0.6 wt % molybdenum;
- from about 0.01 wt % to about 0.05 wt % boron;
- from about 0.005 wt % to about 0.1 wt % zirconium;
- and
- balance nickel and incidental impurities;
- wherein:
- the composition has a solidus temperature in a range of from about 2380° F. to about 2460° F.;
- and/or
- the composition has solidification window greater than 55° F.
(canceled)
(canceled)
(canceled)
(canceled)
A method of using a composition, the composition comprising:
- from about 0.2 wt % to about 0.7 wt % hafnium;
- from about 4.0 wt % to about 5.5 wt % tantalum;
- from about 8 wt % to about 10 wt % tungsten;
- from about 0.06 wt % to about 0.1 wt % carbon;
- from about 9 wt % to about 10 wt % cobalt;
- from about 8 wt % to about 8.7 wt % chromium;
- from about 5.25 wt % to about 5.75 wt % aluminum;
- from about 0.5 wt % to about 1.5 wt % titanium;
- from about 0.4 wt % to about 0.6 wt % molybdenum;
- from about 0.01 wt % to about 0.05 wt % boron;
- from about 0.005 wt % to about 0.1 wt % zirconium;
- and
- balance nickel and incidental impurities,
- wherein:
- the composition has a solidus temperature in a range of from about 2380° F. to about 2460° F.;
- and/or
- the composition has solidification window greater than 55° F.;
- wherein the method comprises using the composition for a purpose selected from the group consisting of welding, additive manufacturing, metal casting, coating, repairing, powder metallurgy, and combinations thereof.
An article comprising a composition, the composition comprising:
- from about 0.2 wt % to about 0.7 wt % hafnium;
- from about 4.0 wt % to about 5.5 wt % tantalum;
- from about 8 wt % to about 10 wt % tungsten;
- from about 0.06 wt % to about 0.1 wt % carbon;
- from about 9 wt % to about 10 wt % cobalt;
- from about 8 wt % to about 8.7 wt % chromium;
- from about 5.25 wt % to about 5.75 wt % aluminum;
- from about 0.5 wt % to about 1.5 wt % titanium;
- from about 0.4 wt % to about 0.6 wt % molybdenum;
- from about 0.01 wt % to about 0.05 wt % boron;
- from about 0.005 wt % to about 0.1 wt % zirconium;
- and
- balance nickel and incidental impurities;
- wherein:
- the composition has a solidus temperature in a range of from about 2380° F. to about 2460° F.;
- and/or
- the composition has solidification window greater than 55° F.