Method for producing grain-oriented electrical steel sheet, and induction heating device
AssigneeJfe Steel Corporation
InventorsYusuke SHIMOYAMA, Yukihiro SHINGAKI, Takashi TERASHIMA
Life of this patent
Estimating the term…
Loading patent…
AssigneeJfe Steel Corporation
InventorsYusuke SHIMOYAMA, Yukihiro SHINGAKI, Takashi TERASHIMA
Estimating the term…
A method for producing a grain-oriented electrical steel sheet is disclosed including hot rolling a steel material to obtain a hot-rolled sheet, subjecting the hot-rolled sheet to one cold-rolling step, or two or more cold-rolling steps with intermediate annealing interposed between each cold-rolling step so as to obtain a cold-rolled sheet with a final thickness, and subjecting the cold-rolled sheet to decarburization annealing which also serves as primary recrystallization annealing and then to finishing annealing, in which the decarburization annealing includes a heating step in which the steel sheet is rapidly heated at an average heating rate of 250° C./s or more from 400° C. to a temperature T(° C.) of 700 to 900° C. and then held at a heating rate of ⅔ of the average heating rate or less in any of temperature ranges between 500° C. and 700° C. for a time of 0.10 seconds or more but less than 1.00 seconds.
A method for producing a grain-oriented electrical steel sheet, comprising:
Dependencies are inferred from the claim text.