Back to results
US 2026/0078247 A1Published application
Polyolefins compositions obtained from recycled polyolefins
AssigneeBasell Poliolefine Italia S.r.l.
InventorsStefano Spataro, Davide Tartari, Cristina Cova, Claudio Cavalieri
Life of this patent
Estimating the term…
Abstract
A polypropylene composition made from or containing: (a) from 55 wt % to 80 wt % of a crystalline propylene polymer; (b) from 12 wt % to 30 wt % of an elastomeric terpolymer of propylene, ethylene and 1-butene; and (c) from 8 wt % to 25 wt % of recycled polyethylene (r-PE), wherein the percentages of (a), (b) and (c) being referred to the sum of (a), (b) and (c).
Claims15
A polypropylene composition comprising:
- (a) from 55 wt % to 80 wt % of a crystalline propylene polymer, having an amount of isotactic pentads (mmmm), measured by 13C-NMR on the fraction insoluble in xylene at 25° C.,—higher than 97.0 molar % and a polydispersity index ranging from 3 to 15;
- (b) from 12 wt % to 30 wt % of an elastomeric terpolymer of propylene, ethylene and 1-butene, having an amount of recurring units deriving from ethylene measured by 13C-NMR, ranging from 30.0 wt % to 70.0 wt %, and an amount of recurring units deriving from 1-butene, measured by 13C-NMR, ranging from 5.0 wt % to 25.0 wt %;
- wherein, in the blend of components a) and b);
- i) the polymer fraction soluble in xylene at 25° C. of components a)+b) ranging from 15.0 wt % to 30.5 wt %-;
- ii) the polymer fraction soluble in xylene at 25° C. of components a)+b), having an intrinsic viscosity value, measured in tetrahydronaphthalene at 135° C., ranging from 2.5 dl/g to 4.8 dl/g;
- iii) the ethylene derived units content, measured by 13C-NMR, in the fraction soluble in xylene—at 25° C. of components a)+b), ranging from 20.4 wt % to 37.5 wt %;
- iv) the melting point, measured by DSC, of components a)+b) ranging from 148.0° C. to 168° C.;
- and
- v) the melt flow rate (ISO 1133-1 230° C./2.16 kg) of components a)+b), ranging from 0.1 to 10.0 g/10 min;
- and
- (c) from 8 wt % to 25 wt %, of recycled polyethylene (r-PE), having a melt flow rate ((ISO 1133-1 190° C./2.16 Kg) from 0.1 to 10.0 g/10 min and containing an amount of polypropylene inclusions ranging from 1 wt % to 15 wt %, based upon the total r-PE component;
- wherein the whole composition having a value of melt flow rate (ISO 1133-1 230° C./2.16 kg) ranging from 0.1 to 10.0 g/10 min;
- and
- the percentages of (a), (b) and (c) being referred to the sum of (a), (b) and (c).
11 more elements
Dependencies are inferred from the claim text.