A method for producing a metal composite hydroxide that contains nickel, manganese, and tungsten and optionally cobalt and element M and has a ratio of number of atoms of the respective metal elements represented by Ni:Mn:Co:W:M=x:y:z:a:b (x+y+z=1, 0.3≤x≤0.95, 0.05≤y≤0.55, 0≤z≤0.4, 0<a≤0.1, 0≤b≤0.1, and M is one or more elements selected from Mg, Ca, Al, Ti, V, Cr, Zr, Nb, Mo, Hf, and Ta), the method comprising:
- a first crystallization process of obtaining first metal composite hydroxide particles by supplying a first raw material aqueous solution containing at least one among the metal elements and an ammonium ion donor to a reaction tank, adjusting a pH of a reaction aqueous solution in the reaction tank, and performing a crystallization reaction;
- and
- a second crystallization process of forming a tungsten-concentrated layer on a surface of the first metal composite hydroxide particles and obtaining second metal composite hydroxide particles by supplying a second raw material aqueous solution containing at least one among the metal elements and a more amount of tungsten than the first raw material aqueous solution and an ammonium ion donor to a reaction aqueous solution containing the first metal composite hydroxide particles, adjusting a pH of the reaction aqueous solution, and performing a crystallization reaction.