US 2026/0062587 A1Published application
Solvent-free polyurethane slurry and preparation method thereof, and environmental-friendly resin-coated protective gloves and preparation method thereof
AssigneeWonderGrip(CHINA)CO., Ltd.
InventorsGuoda Dai, Menglu Dai, Genkai Watanabe, Wei Wen
Life of this patent
Estimating the term…
Abstract
Provided are a solvent-free polyurethane (PU) slurry and a preparation method thereof. Also provided are environmental-friendly resin-coated protective gloves and a preparation method thereof. The solvent-free PU slurry includes a component A and a component B, with a mass ratio of the component A to the component B ranging from 100:67 to 100:93.
Claims20
A solvent-free polyurethane (PU) slurry, comprising:
- a component A;
- and
- a component B;
- wherein a mass ratio of the component A to the component B ranges from 100:67 to 100:93;
- wherein the component A comprises the following raw materials in parts by mass:
- 67 parts to 93 parts of a polyoxypropylene tetraol, 7 parts to 24 parts of a hydroxy acrylate, 0.3 parts to 5 parts of an alcohol chain extender, 0.7 parts to 7 parts of a photoinitiator, 0.03 parts to 0.7 parts of a delayed-action catalyst, and 0.03 parts to 0.8 parts of a foam stabilizer;
- and
- wherein the component B comprises the following raw materials in parts by mass:
- 21 parts to 43 parts of a polyoxypropylene diol, 12 parts to 25 parts of a double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of a polyisocyanate, and 0.008 parts to 0.05 parts of a polymerization inhibitor.
6 more elements
A method for preparing a solvent-free PU slurry, the method comprising:
- mixing a polyoxypropylene tetraol, a hydroxy acrylate, and an alcohol chain extender to obtain a first mixture;
- subjecting the first mixture to first heating stirring and cooling in sequence;
- adding a foam stabilizer to a resulting cooled product to obtain a second mixture;
- subjecting the second mixture to second heating stirring to obtain a mixture system;
- mixing the mixture system with a photoinitiator and a delayed-action catalyst to obtain a component A;
- mixing a polyisocyanate and a polymerization inhibitor to obtain a third mixture;
- subjecting the third mixture to third heating stirring;
- adding a polyoxypropylene diol and a double-bond-containing terminal hydroxyl polymer to the third mixture;
- subjecting a resulting product to heating reaction and vacuum defoamation in sequence to obtain a component B;
- and
- mixing the component A and the component B to obtain the solvent-free PU slurry;
- wherein a mass ratio of the component A to the component B ranges from 100:67 to 100:93;
- wherein the component A comprises the following raw materials in parts by mass:
- 67 parts to 93 parts of the polyoxypropylene tetraol, 7 parts to 24 parts of the hydroxy acrylate, 0.3 parts to 5 parts of the alcohol chain extender, 0.7 parts to 7 parts of the photoinitiator, 0.03 parts to 0.7 parts of the delayed-action catalyst, and 0.03 parts to 0.8 parts of the foam stabilizer;
- and
- wherein the component B comprises the following raw materials in parts by mass:
- 21 parts to 43 parts of the polyoxypropylene diol, 12 parts to 25 parts of the double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of the polyisocyanate, and 0.008 parts to 0.05 parts of the polymerization inhibitor.
14 more elements
A method for making a resin-coated protective glove, the method comprising:
- preparing a solvent-free polyurethane (PU) slurry that comprises a component A and a component B, wherein a mass ratio of the component A to the component B ranges from 100;
- 67 to 100;
- 93;
- preheating a hand model covered with a glove core;
- coating an anti-penetration agent on a surface of the glove core;
- subjecting a resulting coated glove core to impregnating with the solvent-free PU slurry, ultraviolet (UV)-curing, and drying in sequence;
- and
- then subjecting a resulting dried product to a post-treatment to obtain the resin-coated protective glove;
- wherein the component A comprises the following raw materials in parts by mass:
- 67 parts to 93 parts of a polyoxypropylene tetraol, 7 parts to 24 parts of a hydroxy acrylate, 0.3 parts to 5 parts of an alcohol chain extender, 0.7 parts to 7 parts of a photoinitiator, 0.03 parts to 0.7 parts of a delayed-action catalyst, and 0.03 parts to 0.8 parts of a foam stabilizer;
- and
- wherein the component B comprises the following raw materials in parts by mass:
- 21 parts to 43 parts of a polyoxypropylene diol, 12 parts to 25 parts of a double-bond-containing terminal hydroxyl polymer, 45 parts to 61 parts of a polyisocyanate, and 0.008 parts to 0.05 parts of a polymerization inhibitor.
10 more elements
Dependencies are inferred from the claim text.