Cathode material, preparation method thereof and battery
AssigneeBTR Nano Tech Co., Ltd.
InventorsGuoxue LIU, Jinzhi SHENG, Yu ZHENG, Xiaozhen WU, Shunyi YANG, Youyuan HUANG
Life of this patent
Estimating the term…
Loading patent…
AssigneeBTR Nano Tech Co., Ltd.
InventorsGuoxue LIU, Jinzhi SHENG, Yu ZHENG, Xiaozhen WU, Shunyi YANG, Youyuan HUANG
Estimating the term…
A cathode material, a preparation method thereof and a battery. The cathode material has a chemical formula of LinNi1-x-yMxMnyO2, where 0.9≤n≤1.2, 0<x<1, 0<y<1, and M is selected from Co and/or Al, the cathode material includes first particles with the maximum diameter of ≤1.5 μm and second particles with the maximum diameter of ≥2.5 μm, by characterizing the first particles through energy dispersive spectroscopy (EDS), an average value of molar ratios of Ni element and Mn element is denoted as R1, and by characterizing the second particles through energy dispersive spectroscopy (EDS), an average value of molar ratios of Ni element and Mn element is denoted as R2, where 0<R2−R1. Regarding the cathode material, the specific capacity and the initial efficiency performance as well as the structural stability and the cycle performance of the cathode material are effectively improved.
A cathode material, having a chemical formula of LinNi1-x-yMxMnyO2, wherein 0.9≤n≤1.2, 0<x<1, 0<y<1, and M is selected from Co and/or Al,
A cathode material precursor, wherein the cathode material precursor has a chemical formula of NiaMbMncO, wherein 0<a<1, 0<b<1, 0<c<1, and a+b+c=1, and M is selected from Co and/or Al, and wherein by testing through XRD, the cathode material precursor has diffraction peaks both at 35.4°±1° and at 43.3°±1°.