Polymeric Back Interface Layer for CdTe/CdSeTe Solar Cells
AssigneeThe University of Toledo
InventorsRandall J. Ellingson, Scott Lambright, Abasi Abudulimu, Michael Heben, Robert Earl Cannon, Adam Phillips
Life of this patent
Estimating the term…
Abstract
Photovoltaic devices, and methods of making the same, are described. The photovoltaic devices includes a hole-transport layer which includes poly(9-vinylcarbazole) (PVK).
Claims20
A photovoltaic device comprising:
- a front contact;
- one or more layers on the front contact including a photovoltaic heterojunction, the photovoltaic heterojunction comprising an absorber layer, wherein the absorber layer comprises cadmium and tellurium;
- a hole transport layer on the absorber layer, wherein the hole transport layer comprises poly(9-vinylcarbazole) (PVK);
- and
- a back contact on the hole transport layer.
2 more elements
A photovoltaic device comprising:
- a first electrically conductive layer having n-type conductivity;
- an absorber layer comprising cadmium and tellurium on the first electrically conductive layer, the absorber layer forming a photovoltaic heterojunction with either the first electrically conductive layer or an additional layer between the first electrically conductive layer and the absorber layer;
- and
- a back contact structure on the absorber layer comprising a hole transport material and a second electrically conductive layer, wherein the hole transport material comprises poly(9-vinylcarbazole) (PVK) and the second electrically conductive layer has p-type conductivity.
1 more element
A method of making a photovoltaic device, the method comprising:
- exposing a layer stack having an absorber layer material comprising cadmium and tellurium deposited on a surface thereof to a bath comprising KOH;
- thermally annealing the layer stack at a first elevated temperature for a first period of time;
- depositing poly(9-vinylcarbazole) (PVK) from a solution onto the surface;
- and
- thermally annealing the layer stack at a second elevated temperature for a second period of time, wherein the second elevated temperature is 150° C. or less.
2 more elements