Back to results
US 2026/0005028 A1Published application
Pulsing deposition using fast response mfc
AssigneeApplied Materials, Inc.
InventorsZheyuan Chen, Jianxin Lei, Allyson N. Vu
Life of this patent
Estimating the term…
Abstract
Methods for forming work function layers (e.g., titanium nitride work function layers) for transistors are described. The methods energizing a process gas disposed in an inner volume of a processing chamber to create a plasma, and pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the work function layer on the substrate surface.
Claims20
A method of forming a work function layer for a transistor, the method comprising:
- energizing a process gas disposed in an inner volume of a processing chamber to create a plasma, the processing chamber having a sputtering target and the plasma causing atoms to eject from the sputtering target toward a substrate surface;
- and
- pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the work function layer on the substrate surface, the fast response mass flow controller having an ON response delay and an OFF response delay independently less than or equal to 0.25 seconds at a flow rate in the range of 5 sccm to 100 sccm.
A method of forming a titanium nitride work function layer for a transistor, the method comprising:
- flowing a process gas comprising argon and nitrogen into an inner volume of a processing chamber comprising a titanium target and a substrate with a substrate surface;
- energizing the process gas to create a plasma in the inner volume to cause titanium atoms to eject from the sputtering target toward the substrate surface;
- and
- pulsing the process gas between a poison regime and a metallic regime using a fast response mass flow controller to deposit the titanium nitride work function layer on the substrate surface,
- wherein the fast response mass flow controller having an ON response delay and an OFF response delay independently less than or equal to 0.15 seconds at a flow rate in the range of 5 sccm to 100 sccm,
- wherein the metallic regime has a nitrogen flow rate in the range of 20 sccm to 30 sccm, and the poison regime has a nitrogen flow rate in the range of 25 sccm to 35 sccm and is greater than the nitrogen flow rate of the metallic regime.
3 more elements