Polylactide-peroxide masterbatches and branching process
OwnerAdegbola Adenusi, Marc Flodquist +2inventors
InventorsAdegbola Adenusi, Marc Flodquist, Nemat Hossieny, Jed Richard Randall
Life of this patent
Estimating the term…
Abstract
Solidified polylactide-peroxide masterbatches contain at least 50% of a linear amorphous grade polylactide resin and 1 to 30 parts, per 100 parts by weight of the polylactide, of a peroxide having a half-life of at least 50 seconds at 180° C. The masterbatches are made by combining the polylactide resin and peroxide at a temperature of 80 to 170° C. and then cooling the resulting mixture. The masterbatch is useful for preparing branched and/or crosslinked polylactides.
Claims19
A solidified polylactide-peroxide masterbatch comprising a thermoplastic resin phase comprising at least 50% by weight of a linear amorphous grade polylactide resin based on the weight of the thermoplastic resin phase and 1 to 30 parts by weight per 100 parts by weight of the thermoplastic resin phase of a peroxide, the peroxide having a half-life of at least 50 seconds at 180° C. dissolved or dispersed in the thermoplastic resin phase.
A method for making a solidified polylactide-peroxide masterbatch, comprising the steps of
- i) combining a) one or more thermoplastic resins, the thermoplastic resins comprising at least 50% by weight of a starting linear amorphous grade polylactide resin with b) 1 to 30 parts by weight, per 100 parts by weight of the starting amorphous grade PL(Original) A resin, of a peroxide, the peroxide having a half-life of at least 50 seconds at 180° C. and mixing the starting linear amorphous grade polylactide and the peroxide at a temperature of 80 to 170° C. to produce a solution or dispersion of the one or more peroxides in the thermoplastic resins, and
- ii) cooling the solution or dispersion to a temperature of at most 40° C. to produce the solidified polylactide-peroxide masterbatch.
Dependencies are inferred from the claim text.