Lithium transition metal oxide and precursor particulates and methods
AssigneeNovonix Battery Technology Solutions Inc.
InventorsLituo ZHENG, Mark OBROVAC
Life of this patent
Estimating the term…
Abstract
Improved methods for preparing lithium transition metal oxide particulate such as lithium nickel metal cobalt oxide (“NMC”) for use in lithium batteries and other applications are disclosed. The lithium transition metal oxide particulate is prepared from appropriate transition metal oxide and Li compound precursors mainly using dry, solid state processes including dry impact milling and heating. Further, novel precursor particulates and novel methods for preparing precursor particles for this and other applications are disclosed.
Claims21
1-37. (canceled)
A method of making a lithium transition metal oxide active material with an O3 crystal structure, an average particle size greater than 1 μm and having a formula Li1+x[(NinMnmCOc)1−aAa]1−xO2 wherein:
- A is a metal dopant;
- and
- x, n, m, c and a are numbers wherein:
- -
- 0.03
- ≤
- x
- ≤
- 0.06
- ;
- n
- +
- m
- +
- c
- =
- 1
- ;
- n
- ≥
- 0.05
- ;
- m
- ≥
- 0
- ;
- c
- ≥
- 0
- ;
- 0
- ≤
- a
- ≤
- 0.05
- ;
- and
- m
- +
- c
- +
- a
- ≥
- 0.05
- .
- wherein A is a metal dopant that is not Ni, Mn, Co, and Li;
- the method comprising:
- obtaining a source of Ni, a source of Mn, a source of Co, and a source of A according to the formula;
- wherein the source of Ni, the source of Mn, the source of Co, and the source of A are in the form of metal oxides, hydroxides or carbonates;
- preparing a mixture comprising an amount of the source of Ni, the source of Mn, the source of Co, the source of A, and an amount of a Li compound;
- wherein the Li compound is selected from the group consisting of Li oxide, Li hydroxide, Li carbonate and mixtures thereof;
- wherein the total number of moles of Ni in the mixture to the total number of moles of Mn in the mixture to the total number of moles of Co in the mixture to the total number of moles of A in the mixture is equal to n:m:c:a;
- wherein the total number of moles of Li in the mixture is greater or equal to the amount according to the formula;
- and
- heating the mixture at a temperature greater than 700° C. in oxygen and/or air to produce the lithium transition metal oxide active material with the O3 crystal structure.
A method of making a lithium transition metal oxide active material with an O3 crystal structure, an average particle size greater than 1 μm and having a formula Li1+x[(NinMnmCOc)1−aAa]1−xO2 wherein:
- A is a metal dopant;
- and
- x, n, m, c and a are numbers wherein:
- -
- 0.03
- ≤
- x
- ≤
- 0.06
- ;
- n
- +
- m
- +
- c
- =
- 1
- ;
- n
- ≥
- 0.05
- ;
- m
- ≥
- 0
- ;
- c
- ≥
- 0
- ;
- 0
- ≤
- a
- ≤
- 0.05
- ;
- and
- m
- +
- c
- +
- a
- ≥
- 0.05
- .
- wherein A is a metal dopant that is not Ni, Mn, Co, and Li;
- the method comprising:
- dry mixing metal oxides, hydroxides or carbonates according to the formula to produce a final mixture;
- and
- heating the final mixture at a temperature greater than 700° C. in oxygen and/or air to produce the lithium transition metal oxide active material with the O3 crystal structure.
Dependencies are inferred from the claim text.