Process for manufacturing parts by laser cutting metallic-glass strips
AssigneePatek Philippe SA Geneve
InventorsColine JIGUET, Laura WAGNIERES
Life of this patent
Estimating the term…
Abstract
Disclosed is a process for cutting a metallic-glass strip, comprising applying to the strip a pulsed laser beam of wavelength shorter than or equal to 555 nanometers, the pulsed laser beam being formed of a succession of pulses each having a duration shorter than 10 picoseconds, and advantageously shorter than 1 picosecond, the crystallization temperature of the metallic glass being below 500° C., and the light energy of the laser beam incident on the strip being comprised between 1 and 10 microjoules per pulse.
Claims20
A process for cutting a metallic-glass strip, the method comprising:
- applying a pulsed laser beam of wavelength shorter than or equal to 555 nanometers to the metallic-glass strip, the pulsed laser beam being formed of a succession of pulses each having a duration shorter than 10
- wherein metallic glass of the metallic-glass strip has a crystallization temperature below 500° C., and
- light energy of the laser beam incident on the strip is comprised between 1 and 10 microjoules per pulse.
The process for cutting the metallic-glass strip, further comprising:
- providing equipment comprising
- at least one laser configured to produce the pulsed laser beam of wavelength shorter than or equal to 555 nanometers, and
- an attenuator of the laser beam configured to adjust a quantity of the light energy of the incident laser beam;
- providing a metallic-glass sample to be cut;
- adjusting the attenuator such that the light energy of the laser beam incident on the strip is comprised between 1 and 10 microjoules per pulse when the crystallization temperature of the metallic glass of the metallic-glass sample to be cut is below 500° C., and such that the light energy of the laser beam incident on the strip is comprised between 15 and 80 microjoules per pulse when the crystallization temperature of the metallic glass of the metallic-glass sample to be cut is above 500° C.;
- and
- cutting the metallic-glass strip by applying the laser beam to the metallic-glass sample, the light energy of which has been adjusted by the adjusting the attentuator, by one of:
- (i) the applying the pulsed laser beam of wavelength shorter than or equal to 555 nanometers to the metallic-glass strip when the metallic glass of the metallic-glass strip has the crystallization temperature below 500° C., and (ii) applying said laser beam to the metallic-glass sample, the light energy of which is comprised between 15 and 80 microjoules per pulse, when the metallic glass of the metallic-glass strip has the crystallization temperature above 500° C.
Dependencies are inferred from the claim text.