Additive manufacturing systems and methods for the same
AssigneeAdditive Technologies, LLC dba ADDiTEC
InventorsPatrick Y. MAEDA, Daniel BULLARD, Dogan TIMUCIN
Life of this patent
Estimating the term…
Abstract
An additive manufacturing device includes a stage configured to support a substrate. The device also includes a printhead disposed above the stage. The printhead is configured to heat a build material to a molten build material and to deposit the molten build material on the substrate in the form of droplets to fabricate an article. The device also includes a controlled heating and ablation system disposed proximal the printhead. The controlled heating and ablation system is configured to heat the substrate and ablate oxides on a surface of the substrate.
Claims20
A method for fabricating an article with an additive manufacturing device, the method comprising:
- heating a metal build material in a printhead to produce a molten metal build material;
- ejecting the molten metal build material from the printhead towards a substrate, which forms a stack of layers of the metal build material on the substrate;
- and
- ablating metal oxides formed on a top layer of the stack of layers of the metal build material with a controlled heating and ablation system, wherein a laser intensity of the controlled heating and ablation system is higher than an ablation threshold of the metal oxides and lower than a melting threshold of the metal build material.
A method for fabricating an article with an additive manufacturing device, the method comprising:
- heating a metal build material to produce a molten metal build material using a printhead;
- depositing the molten metal build material on a substrate in the form of droplets to form a stack of layers of the metal build material;
- and
- heating the layers, which ablates metal oxides on a top layer of the stack of layers, using a controlled heating and ablation system, wherein an intensity of a laser of the controlled heating and ablation system is higher than an ablation threshold of the metal oxides and lower than a melting threshold of the metal build material.
A method for fabricating an article with an additive manufacturing device, the method comprising:
- heating a metal build material to produce a molten metal build material using a printhead;
- depositing the molten metal build material on a substrate in the form of droplets to form a layer of the metal build material;
- and
- heating the layer, which ablates metal oxides on the layer, using a controlled heating and ablation system, wherein an intensity of a laser of the controlled heating and ablation system is higher than an evaporation threshold of cupric oxide (CuO) and lower than a melting threshold of the layer, and wherein
- a power of the laser is from about 40 watts (W) to about 1500 W,
- an irradiance of the laser is from about 1 W/cm2 to about 10,000 W/cm2,
- a wavelength of the laser is from about 355 nm to about 1200 nm,
- a fluence (F) of the laser is from about 0.1 J/cm2 to about 50 J/cm2,
- a pulse energy of the laser is from about 1 microjoule (μJ) to about 50 millijoules (mJ),
- a pulse repetition rate of the laser is from about 5 kHz to about 250 MHZ,
- a pulse width of the laser is from about 0.5 ns to about 100 ms, and
- a pulse duration of the laser is lower than a thermal relaxation time of the metal layer to minimize a temperature increase of the metal layer, and
- an area on the surface that is heated by the laser has a diameter of from about 0.025 mm to about 2.0 mm;
- monitoring a temperature of the layer;
- and
- adjusting the power, the irradiance, the wavelength, the fluence, the pulse energy, the pulse repetition rate, the pulse duration, and the area in response to the temperature of the layer.
Dependencies are inferred from the claim text.