Wear resistant steel with high hardness and good toughness which keeps hardened after hard facing and tungsten carbide tile brazing
OwnerShane Xinyang LIinventor
Life of this patent
Estimating the term…
Abstract
The present invention relates to a steel composition consisting of Carbon (C) 0.15-1.50%, Silicon (Si) 0.9-3.5%, Manganese (Mn) 1.0-4.0%, Chromium (Cr) 0.6-5.0%, Molybdenum (Mo) 0.05-0.60%, Vanadium (V) 0.05-6.00%, Tungsten (W) 0.05-10.00%, the balance being Iron (Fe) and unavoidable impurities. The steel composition retains high hardness after hard facing and tungsten carbide tile brazing, allowing for application to farming and mining industries and the like.
Claims17
1-17. (canceled)
A steel composition consisting of carbon 0.20-0.30%, silicon 2.6-2.8%, manganese 2.0-2.3%, chromium 2.7-3.0%, molybdenum 0.15-0.25, vanadium 0.40-0.70%, boron, sulphur, and phosphorous 0-.0.04%, and remainder iron, wherein the steel composition comprises a hardness value in the range 57-63 HRC and a toughness of at least 32 J.
A steel composition consisting of carbon 0.30-0.40%, silicon 2.60-2.80%, manganese 2.0-3.0%, chromium 2.5-3.0%, molybdenum 0.3-0.5%, tungsten 6-8%, vanadium 0.20-0.40%, boron, sulphur,and phosphorous 0-.0.04%, and remainder iron, wherein the steel composition comprises a hardness of about 57-63 HRC and a toughness of at least 32 J.
Dependencies are inferred from the claim text.