Sulphide based lithium-ion conducting solid electrolyte and methods for the production thereof
AssigneeUmicore AG & Co. KG
InventorsAntoine BREHAULT, Pol BRIANTAIS, Yann GUIMOND, Tom KREKELS
Life of this patent
Estimating the term…
Abstract
The present invention relates to solid materials which are obtainable by melt-quenching mixtures of lithium sulphide, boron sulphide and boron oxide, thereby forming a glassy solid which is suitable for use as a lithium-ion conducting electrolyte. These sulphide based lithium-ion conducting solid electrolytes exhibit a large thermal stability as supported by the large ΔTx, in particular a ΔTx of more than 100° C.
Claims19
1-18. (canceled)
A solid material having a composition according to general formula (I)
- Li2c+dB2a+2bS3a+cO3bXd (I)
- wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
- a is within the range of 0.03 to 0.1;
- b is within the range of 0 to 0.04;
- c is within the range of 0.12 to 0.26;
- and
- d is within the range of 0.001 to 0.14.
A solid material, which is obtainable by melt-quenching a mixture of A and B,
- wherein the molar ratio of A and B in the mixture before quenching is within the range of 60:40 to 99:1;
- wherein component A is according to general formula (II)
- xLi2S-yB2S3-zB2O3 (II)
- wherein
- x is within the range of 55 to 85;
- y is within the range of 15 to 45;
- z is within the range of 0 to 15;
- x+y+z=100;
- and
- wherein component B is LiX, wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof.
A method for preparing a solid material, comprising the steps of:
- (i) providing the following precursors:
- Li2S;
- B2S3 and/or both of boron and sulfur;
- optionally B2O3;
- and
- LiX wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
- (ii) preparing a mixture comprising the precursors provided in step (i) wherein
- in said mixture the molar ratio of the elements Li, S, B, O and X matches the general formula (I):
- Li2c+dB2a+2bS3a+cO3bXd (I),
- wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
- a is within the range of 0.03 to 0.1;
- b is within the range of 0 to 0.04;
- c is within the range of 0.12 to 0.26;
- and
- d is within the range of 0.001 to 0.14;
- or
- in said mixture the molar ratio of A and B in the mixture is within the range of 60:40 to 99:1;
- wherein component A is according to general formula (II):
- xLi2S-yB2S3-zB2O3 (II),
- wherein x is within the range of 55 to 85;
- y is within the range of 15 to 45;
- z is within the range of 0 to 15;
- x+y+z=100;
- and
- wherein component B is LiX, wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
- (iii) heat-treating the mixture prepared in step (ii) to obtain a melt;
- and
- (iv) quenching the melt obtained in step (iii) to obtain the solid material.
Dependencies are inferred from the claim text.