A positive electrode active material comprises a first active material, and a second active material having a greater average particle size than the first active material. Each of the first active material and the second active material is a lithium-(transition metal) composite oxide including Ni at 75 mol % or more relative to a total number of moles of metallic element except Li. The first active material is a single particle, or a secondary particle consisting of 2 to 10 primary particles aggregated together, and the second active material is a secondary particle consisting of at least 50 primary particles aggregated together. A crystallite size L1 of the first active material is 80,000 Å or more. A crystallite size L2 of the second active material is 2,000 Å or less. A crystallite size ratio of the first active material (L003/L104) is from 1.60 to 2.0.
A positive electrode active material comprising:
Dependencies are inferred from the claim text.