Electrode active material, electrode mixture, electrode layer, battery, and method for producing these
AssigneeToyota Jidosha Kabushiki Kaisha
InventorsMitsutoshi OTAKI, Masafumi Nose
Life of this patent
Estimating the term…
Abstract
A main object of the present disclosure is to provide an electrode active material of which volume change due to charge and discharge is small. The present disclosure achieves the object by providing an electrode active material including a silicon clathrate II type crystal phase, wherein a void is included inside a primary particle; and a void amount P1 of a void with a pore diameter of 5 nm or less is 0.015 cc/g or more and 0.05 cc/g or less.
Claims20
An electrode active material comprising a silicon
- clathrate II type crystal phase, wherein
- a void is included inside a primary particle;
- and
- a void amount P1 of a void with a pore diameter of 5 nm or less is 0.015 cc/g or more and 0.05 cc/g or less.
An electrode layer to be used in a battery, the electrode layer comprising:
- an electrode active material including a silicon clathrate II type crystal phase and a void inside a primary particle, wherein
- a void amount Q1 of a void with a pore diameter of 5 nm or less is 0.008 cc/g or more and 0.04 cc/g or less.
A method for producing an electrode active material, the method comprising:
- an alloying step of obtaining a Na—Si alloy by bringing a Na source and a Si source into reaction;
- a burning step of burning the Na—Si alloy to decrease Na amount in the Na—Si alloy and form a precursor active material including a silicon clathrate II type crystal phase;
- and
- a liquid treatment step of performing a liquid treatment to the precursor active material using a hydrofluoric acid, wherein
- a concentration of hydrogen fluoride in the hydrofluoric acid is 3 weight % or more;
- and
- a treatment time in the liquid treatment step is 3 hours or more and less than 24 hours.
Dependencies are inferred from the claim text.